Borlink™ LH4201R

About
Borlink LH4201R is a crosslinkable natural polyethylene compound, specially designed for insulation of energy cables. Applications Borlink LH4201R is intended for insulation of XLPE power cables with rated voltages up to 72 kV. It is designed for cable constructions with bonded insulation shields. Specifications Borlink LH4201R meets the applicable requirements as below when processed using sound extrusion practices and testing procedures Cenelec HD 620 S1, Part 1, table 2A, DIX 3 to 14 DIN VDE 0276-620 GOSTR 55025-2012 IEC 60502-2 IEC 60840 Special Features Borlink LH4201R is a ready-to-use natural co-polymer compound. It provides superior electrical performance (polymer WTR XLPE) meeting the most stringent wet ageing requirements. It offers excellent scorch resistance and long production runs. Borlink LH4201R cleanliness level is assured through the Borealis quality control system.&&

Product Description
SupplierBorealis AG
GenericPE
Material StatusCommercial: Active
FeaturesGood Electrical Properties,Crosslinked,High Heat Resistance,Heat Stabilized
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe
Process MethodsExtrusion

Technical Data
PHYSICALNominal valueUnitTest method
Density0.924g/cm³ISO 1183
Melt Flow Rate
190℃,2.16kg2.8g/10minISO 1133
Moisture< 200ppmKarl Fisher

MECHANICALNominal valueUnitTest method
tensile strength> 17.0MPaISO 527-2/250
Tensile strain
fracture> 450%ISO 527-2/250

THERMALNominal valueUnitTest method
thermosetting IEC 60811-507
Elongation under load: 200 ℃75%IEC 60811-507
Permanent deformation: 200 ℃5.0%IEC 60811-507

Aging performanceNominal valueUnitTest method
Change in Tensile Strain at Break in Air(135℃,168 hr)< 20%IEC 60811-401

Electrical performanceNominal valueUnitTest method
Volume resistivity> 1.0E+16ohms·cmIEC 60093
Dielectric strength> 22kV/mmIEC 60243-1
Dielectric constant
50 Hz2.30 IEC 60250
Dissipation factor
50 Hz5.0E-4 IEC 60250

Supplementary informationNominal valueUnitTest method
Methanol Wash< 500ppmInternal Method
Monsanto ODR30.0 to 38.0dN·mASTM D2084

Process Conditions
ExtrusionNominal valueUnitTest method
Melt temperature125 to 135°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. 0.20 MPa
3. 50 Hz
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.