About |
---|
HDB0763 is a high density polyethylene homopolymer, developed specifically for blow molding food containers. It exhibits excellent processing characteristics and extremely low odor in the finished container. This material meets the Food and Drug Administration requirements of 21 CFR 177.1520. Typical Applications: Blow molded small volume containers for dairy products, yogurt, juice and other liquid food packing. Process: Blow Molding Injection Blow Molding&& |
Product Description | |
---|---|
Supplier | Braskem |
Generic | HDPE |
Material Status | Commercial: Negative |
Features | Excellent Processability,Food contact compliance,Low odor,Homopolymer |
Availabilitys | North America,Latin America |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.963 | g/cm³ | ASTM D4883 |
Melt Flow Rate | |||
190℃,2.16kg | 0.72 | g/10min | ASTM D1238 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Impact strength of cantilever beam notch | 190 | J/m | ASTM D256 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 84.0 | ℃ | ASTM D648 |
Embrittlement temperature | < -75.0 | ℃ | ASTM D746 |
Vicat Softening Temp | 132 | ℃ | ASTM D1525 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s D | 66 | ASTM D2240 | |
tensile strength | |||
yield | 31.0 | MPa | ASTM D638 |
Tensile strain | |||
fracture | 600 | % | ASTM D638 |
Bending modulus | ASTM D790 | ||
2% secant | 1240 | MPa | ASTM D790 |
tangent | 1550 | MPa | ASTM D790 |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |