About |
---|
IC32 is a linear low-density polyethylene, with narrow molecular weight, produced by solution process, for injection molding. It offers good fluidity, excellent flexibility, tenacity and low warpage. It contains special antioxidant additives. Application: Resin has been specifically developed for lids molding injection, house appliances and master batch production.&& |
Product Description | |
---|---|
Supplier | Braskem |
Generic | Linear low density polyethylene |
Material Status | Commercial: Active |
Features | Low warping,Good flexibility,Inoxidizability,Weight distribution |
Availabilitys | Latin America,Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.924 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
190℃,2.16kg | 29 | g/10min | ASTM D1238 |
ESCR(Environmental Stress Cracking Resistance) | |||
50 ℃, 2.00 mm, 10% non-ionic surfactant, molded, F50 | < 1.00 | hr | ASTM D1693 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | ASTM D638 | ||
Yield, molding | 12.0 | MPa | |
Fracture, molded | 10.0 | MPa | |
Tensile strain | |||
Fracture, molded | 250 | % | ASTM D638 |
Bending modulus | |||
23℃ | 320 | MPa | ASTM D747 |
Bending modulus | |||
1% cut, molded | 370 | MPa | ASTM D790 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Embrittlement temperature | < -70.0 | ℃ | ASTM D746 |
Vicat Softening Temp | 95.0 | ℃ | ASTM D1525 1 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Barrel rear temperature | 150 to 200 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |