About |
---|
BRASKEM C715-12NHP Polypropylene Resin is an impact copolymer for various injection moulding applications. BRASKEM C715-12NHP Polypropylene Resin has a good balance of mechanical properties featuring high stiffness and excellent impact strength, also at low temperatures. BRASKEM C715-12NHP Polypropylene Resin is a medium flow impact copolymer exhibiting a higher rigidity impact balance than conventional impact copolymers at similar flow. Applications: Containers, baskets, pails, caps & closures and other consumer applications General automotive Process: Injection moulding&& |
Product Description | |
---|---|
Supplier | Braskem |
Generic | PP homopolymerization |
Material Status | Commercial: Active |
Availabilitys | Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.900 | g/cm³ | ISO 1183 |
Melt Flow Rate | |||
230℃,2.16kg | 12 | g/10min | ISO 1133 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
Yield, injection molding | 24.0 | MPa | ISO 527-2 |
Tensile strain | |||
Yield, injection molding | 8.0 | % | ISO 527-2 |
Bending modulus | |||
injection molding | 1450 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | ||
-20 ℃, injection molding | 4.5 | kJ/m² | ISO 179/1eA |
0 ℃, injection molding | 6.0 | kJ/m² | ISO 179/1eA |
23 ℃, injection molding | 10 | kJ/m² | ISO 179/1eA |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 100 | ℃ | ISO 75-2/B |
Vicat Softening Temp | 152 | ℃ | ISO 306/A |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. Injection Molded |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |