| About |
|---|
| Modified Ethylene Copolymer CAPXIDAN® LG is a modified copolymer produced with a proprietary, patent pending formulation. It is designed to be coextruded over Wood-Plastic Composite (WPC) deckboards to provide moisture, stain and wear resistance, aesthetics, low gloss, durability at elevated temperatures, and unprecedented adhesion to the WPC substrate. CAPXIDAN® LG is a two-component capstock system. The CAPXIDAN® resin should be extruded together with a specific synergistic additive masterbatch in the recommended proportion of 98:2 by weight.&& |
| Product Description | |
|---|---|
| Generic | Ethylene copolymer |
| Material Status | Commercial: Active |
| Features | The fouling resistance,Good bond,Moisture resistance,Copolymer,Good wear resistance,Durability,Low Gloss |
| Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 0.950 | g/cm³ | ASTM D792 |
| Melt Flow Rate | |||
| 190℃,2.16kg | 0.40 | g/10min | ASTM D1238 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Tensile modulus | |||
| 23℃ | 0.207 | MPa | ASTM D638 |
| tensile strength | |||
| yield | 20.0 | MPa | |
| fracture | 20.7 | MPa | |
| Tensile strain | |||
| fracture | 400 | % | ASTM D638 |
| Anti scratch | |||
| 50℃ | Excellent |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Melting peak temperature | 128 | ℃ | ASTM D3418 |
| optical performance | Nominal value | Unit | Test method |
|---|---|---|---|
| gloss | |||
| 60° | < 4 |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 2. 23°C |
| 3. Multifinger scratch-meter |
| 4. Gloss-meter reading |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |