Celcon® M90™

About
Celcon acetal copolymer grade M90TM is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film. This grade provides overall excellent performance in many applications. Chemical abbreviation according to ISO 1043-1: POM Please also see Hostaform® C 9021.&&

Product Description
SupplierCelanese
GenericCopolymer Polyformaldehyde
Material StatusCommercial: Active
AvailabilitysNorth America,Latin America
Process MethodsInjection Molding

Technical Data
MECHANICALNominal valueUnitTest method
Tensile modulus2760MPaISO 527-2/1A/1
tensile strength ASTM D638
yield65.0MPaISO 527-2/1A/50
Yield, -40 ℃94.5MPaASTM D638
Yield, 23 ℃60.7MPaASTM D638
Yield, 71 ℃34.5MPaASTM D638
Tensile strain
yield10%ISO 527-2/1A/50
Tensile Creep Modulus(1 hr)2450MPaISO 899-1
Tensile creep modulus
1000 hr1350MPaISO 899-1
Bending modulus
23℃2550MPaISO 178

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength ISO 179/1eA
-30℃6.0kJ/m²ISO 179/1eA
23℃6.0kJ/m²ISO 179/1eA
Charpy Unnotch Impact strength ISO 179/1eU
-30℃180kJ/m²ISO 179/1eU
23℃190kJ/m²ISO 179/1eU
Impact strength of cantilever beam notch
23℃5.7kJ/m²ISO 180-1A

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed110ASTM D648
1.8 MPa, unannealed101ISO 75-2/A
0.45 MPa, unannealed158ISO 75-2/B
Melting peak temperature165ASTM D3418
Melting temperature165ISO 11357-3
Linear coefficient of thermal expansion
TD1.2E-41/℃ISO 11359-2
MD1.2E-41/℃ISO 11359-2
Effective Thermal Diffusivity0.0485cStInternal Method

Electrical performanceNominal valueUnitTest method
Surface resistivity3.0E+16ohmsIEC 60093
Volume resistivity1.0E+14ohms·cmASTM D257
Volume resistivity8.0E+14ohms·cmIEC 60093

PHYSICALNominal valueUnitTest method
Density1.41g/cm³ASTM D792
Density1.41g/cm³ISO 1183
Melt Flow Rate9.0g/10minASTM D1238
Melt Volume Rate
190℃,2.16 kg8.00cm³/10minISO 1133
Shrinkage rate ISO 294-4
TD1.8%ASTM D955
MD2.2%ASTM D955
TD1.9%ISO 294-4
MD2.0%ISO 294-4
Water absorption rate
Saturation, 23 ℃0.75%ISO 62
Equilibrium, 23 ℃, 50% RH0.20%ISO 62
Density of Melt1.200g/cm³Internal Method
Specific Heat Capacity of Melt2210J/kg/℃Internal Method
Thermal Conductivity of Melt0.16W/m/KInternal Method

Process Conditions
injectionNominal valueUnitTest method
Drying temperature80 to 100°C
Drying time3.0hr
Barrel rear temperature170 to 180°C
Barrel middle temperature180 to 190°C
Barrel front temperature180 to 190°C
Nozzle temperature190 to 200°C
Processing (melt) temperature180 to 200°C
Mold temperature80 to 120°C
Injection pressure60.0 to 120MPa
Injection speedSlow-Moderate 
Hold pressure60.0 to 120MPa
Back pressure0.00 to 4.00MPa
Ejection temperature140°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. 10°C/min
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.