About |
---|
Chemlon® 133 GH is a Polyamide 66 (Nylon 66) material filled with 33% glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Important attributes of Chemlon® 133 GH are: Flame Rated Good Processability Good Toughness Heat Stabilizer High Strength Typical application of Chemlon® 133 GH: Automotive&& |
Product Description | |
---|---|
Supplier | Teknor Apex |
Generic | PA66 |
Material Status | Commercial: Active |
Features | HB,Excellent Processability,Good flexibility,Heat Stabilized,Good Rigidity,Lubricating |
Availabilitys | Asia Pacific,North America,Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.38 | g/cm³ | ASTM D792 |
Molding shrinkage | |||
MD | 0.15 to 0.40 | % | ASTM D955 |
Water Absorption | |||
24hr | 0.90 | % | ASTM D570 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile Strength | 176 | MPa | ASTM D638 |
Tensile Strain | |||
Broken BRK | 3.0 | % | ASTM D638 |
Yield yld | 3.0 | % | ASTM D638 |
Flexural Modulus | 8620 | MPa | ASTM D790 |
Flexural Strength | 276 | MPa | ASTM D790 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Izod Notched Impact strength | |||
23℃ | 110 | J/m | ASTM D256 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature HDT | |||
1.8 MPa, unannealed | 249 | ℃ | ASTM D648 |
Melting temperature | 257 | ℃ | |
Coeff. of linear thermal expansion | |||
MD | 5.0E-5 | 1/℃ | ASTM D696 |
Relative Temperature Index (RTI) | |||
Electrical performance Elec | UL 746 | ||
0.8 mm | 130 | ℃ | UL 746 |
1.5 mm | 130 | ℃ | UL 746 |
3.0 mm | 130 | ℃ | UL 746 |
Strength mechanical performance str | UL 746 | ||
0.8 mm | 130 | ℃ | UL 746 |
1.5 mm | 130 | ℃ | UL 746 |
3.0 mm | 130 | ℃ | UL 746 |
Impact mechanical performance Imp | UL 746 | ||
0.8 mm | 95.0 | ℃ | UL 746 |
1.5 mm | 110 | ℃ | UL 746 |
3.0 mm | 110 | ℃ | UL 746 |
ELECTRICAL | Nominal value | Unit | Test method |
---|---|---|---|
Volume Resistance | 1.0E+14 | ohms·cm | ASTM D257 |
Dielectric Strength | |||
3 mm | 16 | kV/mm | ASTM D149 |
Compared Tracking Index | 600 | V | UL 746 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame Class Rating | |||
0.80 mm | HB | UL 94 | |
Oxygen Index | 25 | % | ISO 4589-2 |
Process Conditions | |||
---|---|---|---|
Injection Molding | Nominal value | Unit | Test method |
Drying Temperature | 79 | °C | |
Maximum Moisture Content | 0.20 | % | |
Suggested Max Regend | 25 | % | |
Rear Temperature Zone 1 | 246 to 257 | °C | |
Middle Temperature Zone 2 | 263 to 274 | °C | |
Front Temperature Zone 3 | 268 to 282 | °C | |
Nozzle temperature | 268 to 282 | °C | |
Melt Temperature | 263 to 282 | °C | |
Mold Temperature | 60 to 93 | °C | |
Injection pressure | 34.5 to 138 | MPa | |
Screw Speed | 60 to 120 | rpm |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |