CYCOLOY™ FR Resin CX2142ME

About
CYCOLOY CX2142ME Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) resin is an improved chemical resistant grade that can be injection molded. This non-chlorinated, non-brominated flame retardant PC/ABS has a UL V0 & 5VB flame rating. CYCOLOY CX2142ME resin an excellent candidate for a wide variety of applications including enclosures for hospital equipment.&&

Product Description
SupplierSABIC
GenericPC+ABS
Material StatusCommercial: Active
FeaturesHigh impact resistance,Good liquidity,Halogen free,Flame Characteristics,Solvent resistance
AvailabilitysNorth America
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.19g/cm³ASTM D792
Melt Flow Rate
260℃,2.16kg23g/10minASTM D1238
Melt Volume Rate
260℃,2.16 kg21.0cm³/10minISO 1133
Shrinkage rate
MD:3.2 mm0.40 to 0.60%Internal Method
Water absorption rate
Saturation, 23 ℃0.20%
Equilibrium, 23 ℃, 50% RH0.10%

MECHANICALNominal valueUnitTest method
Tensile modulus
2900MPaASTM D638
2700MPaISO 527-1-2
tensile strength
yield64.0MPaASTM D638
yield61.0MPaISO 527-2/50
fracture54.0MPaASTM D638
fracture51.0MPaISO 527-2/50
Tensile strain
yield4.0%ASTM D638
yield4.0%ISO 527-2/50
fracture90%ASTM D638
fracture90%ISO 527-2/50
Bending modulus
50 mm span2700MPaASTM D790
2500MPaISO 178
bending strength
100MPaISO 178
Yield, 50 mm span100MPaASTM D790

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
-30℃10kJ/m²
23℃15kJ/m²
Impact strength of cantilever beam notch
-30℃120J/mASTM D256
23℃600J/mASTM D256
-30℃10kJ/m²ISO 180-1A
23℃15kJ/m²ISO 180-1A
Dart impact equipped with measuring instruments
23℃,Total Energy63.0JASTM D3763

THERMALNominal valueUnitTest method
Hot deformation temperature
0.45 MPa, unannealed, 3.2 mm94.0ASTM D648
0.45 MPa, unannealed, 6.4 mm98.0ASTM D648
1.8 MPa, unannealed, 3.2 mm84.0ASTM D648
1.8 MPa, unannealed, 6.4 mm90.0ASTM D648
1.8 MPa, unannealed, 4.0 mm, 64 mm span84.0ISO 75-2/Af
Vicat Softening Temp102ASTM D1525 11
Ball pressure test
73~77℃通过 IEC 60695-10-2
Linear coefficient of thermal expansion
MD:-40~40℃7.5E-51/℃ASTM E831
TD:-40~40℃7.5E-51/℃ASTM E831
TD:-40℃7.5E-51/℃ISO 11359-2
Thermal conductivity coefficient0.20W/m/KISO 8302

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant level
1.20 mmV-0 
2.00 mm5VB 

Process Conditions
injectionNominal valueUnitTest method
Drying temperature80 to 90°C
Drying time3.0 to 4.0hr
Recommended maximum moisture content0.040%
Recommended injection volume30 to 80%
Barrel rear temperature220 to 255°C
Barrel middle temperature220 to 265°C
Barrel front temperature245 to 275°C
Nozzle temperature245 to 275°C
Processing (melt) temperature245 to 275°C
Mold temperature60 to 80°C
Back pressure0.300 to 0.700MPa
Screw speed40 to 70rpm
Vent depth0.038 to 0.076mm

Notes
1. Typical properties: these are not to be construed as specifications.
2. 2.0 in/min
3. Type I, 2.0 in/min
4. 0.051 in/min
5. 0.079 in/min
6. at Yield
7. 80*10*3 sp=62mm
8. 80*10*3 mm
9. 80*10*4 mm
10. Rate A (50°C/h), Loading 2 (50 N)
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.