| About |
|---|
| CYCOLOY™ C5215是一种15%的玻璃纤维增强PC + ABS混合树脂,用于注射成型。 |
| Product Description | |
|---|---|
| Supplier | SABIC |
| Generic | PC+ABS |
| Material Status | Commercial: Active |
| Features | Glass fiber reinforced |
| Availabilitys | Africa & Middle East ,Asia Pacific,Europe |
| Technical Data | |||
|---|---|---|---|
| MECHANICAL | Nominal value | Unit | Test method |
| tensile strength | |||
| Fracture, 5 mm/min | 86 | MPa | ISO 527 |
| Tensile strain | |||
| Fracture, 5 mm/min | 2.5 | % | ISO 527 |
| Tensile modulus | |||
| 1 mm/min | 5910 | MPa | ISO 527 |
| bending strength | |||
| Yield, 2 mm/min | 134 | MPa | ISO 178 |
| Bending modulus | |||
| 2 mm/mim | 4970 | MPa | ISO 178 |
| IMPACT | Nominal value | Unit | Test method |
|---|---|---|---|
| Impact strength of cantilever beam notch | |||
| 23℃ | 70 | J/m | ASTM D256 |
| Notched impact strength of cantilever beam | |||
| 23℃,80*10*3 | 32 | kJ/m² | ISO 180/1U |
| -30℃,80*10*3 | 7 | kJ/m² | ISO 180/1U |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Hot deformation temperature | |||
| 0.45 MPa, unannealed, 3.2 mm | 95 | ℃ | ASTM D648 |
| Vicat Softening Temp | 100 | ISO 306 |
| PHYSICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Density | 1.29 | g/cm³ | ASTM D792 |
| Water absorption rate | |||
| Saturation, 23 ℃ | 0.15 | % | ISO 62 |
| Melt Flow Rate | |||
| 260℃,2.16kg | 20 | g/10min | ASTM D1238 |
| Melt Volume Rate | |||
| 260℃,2.16 kg | 17 | cm³/10min | ISO 1133 |
| FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
|---|---|---|---|
| 94v-1 flame level assessment | 1.5 | mm | UL 94 |
| Process Conditions | |||
|---|---|---|---|
| injection molding | Nominal value | Unit | Test method |
| Drying temperature | 80 – 90 | °C | |
| Drying time | 3 – 4 | hrs | |
| Maximum water content | 0.01 | % | |
| Melt temperature | 250 – 280 | °C | |
| Nozzle temperature | 250 – 280 | °C | |
| Front Section Zone 3 Temperature | 250 – 280 | °C | |
| Temperature in Zone 2 of the middle section | 240 – 280 | °C | |
| Temperature in Zone 1 of the rear section | 230 – 270 | °C | |
| Mold temperature | 80 – 100 | °C | |
| Back pressure | 3 – 9 | MPa | |
| Screw speed | 30 – 150 | rpm | |
| Notes |
|---|
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |