DOW ENDURANCE™ HFDA-0801 BK EHV is a specially formulated semiconductive, vulcanizable compound designed for conductor shield and bonded insulation shield applications in high and extra-high voltage crosslinked polyethylene insulated cables.(1) DOW ENDURANCE™ HFDA-0801 BK EHV has demonstrated compatibility with copper and aluminum conductors. DOW ENDURANCE™ HFDA-0801 BK EHV was specifically developed utilizing a special acetylene carbon black to provide a supersmooth surface to achieve best in class performance and yielding a more perfect interface between the extruded shield and the insulation. As a result, significantly improved cable performance can be expected. Specifications DOW ENDURANCE™ HFDA-0801 BK EHV is designed for use in power distribution cables. Cables with conductor and insulation shielding of DOW ENDURANCE™ HFDA-0801 BK EHV, prepared using sound commercial fabrication practice, would be expected to meet the following specifications: AEIC: CS8, CS9 IEC: 60502, 60840, 62067 ICEA: S-108-720; S-94-649; S-97-682, S-93-639 DIN: VDE 0276-632, 0276-620 BS: 6622 CENELEC: HD620 S1, HD632 S1 ISO 1872-E/BA, KHXY, 23-G200, C40 NF: C33-223, C33-226 UTE: C33-223 (1) DOW ENDURANCE™ HFDA-0801 BK EHV is recommended for use in conjunction with DOW cross-linked polyethylene and tree-retardant cross-linked polyethylene compounds. For other polymer insulation such as EPR and EPDM’s, the user is cautioned to establish the utility of DOW ENDURANCE™ HFDA-0801 BK EHV with each formulation.&&

Product Description
SupplierDOW
Generic热塑性聚酯
Material StatusCommercial: Active
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe

Technical Data
PHYSICALNominal valueUnitTest method
Density1.14g/cm³ASTM D792
ESCR(Environmental Stress Cracking Resistance)
100% non-ionic detergent, F0> 504hrASTM D1693

MECHANICALNominal valueUnitTest method
tensile strength14.5MPaASTM D638
Tensile strain
fracture200%ASTM D638

Aging performanceNominal valueUnitTest method
Tensile strength retention rate
1 week,150℃98%ASTM D638
Elongation retention rate
1 week,150℃90%ASTM D638

THERMALNominal valueUnitTest method
Embrittlement temperature-40.0ASTM D746

Electrical performanceNominal valueUnitTest method
Volume resistivityASTM D991
23℃15ohms·cm
90 ℃60ohms·cm
130 ℃65ohms·cm

Process Conditions
ExtrusionNominal valueUnitTest method
Drying temperature60.0 to 70.0°C
Drying time< 6.0hr
Melt temperature121 to 140°C

Notes
1. Typical properties: these are not to be construed as specifications.
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.