About |
---|
Eastar™ Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar™ Copolyester DN011 contains a mold release. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®. The GREENGUARD INDOOR AIR QUALITY CERTIFIED® Mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products. This product has been CRADLE TO CRADLE CERTIFIED(cm) The CRADLE TO CRADLE CERTIFIED(cm) Mark is a registered certification mark used under license through McDonough Braungart Design Chemistry (MBDC). MBDC is a global sustainability consulting and product certification firm. The CRADLE TO CRADLE® framework moves beyond the traditional goal of reducing the negative impacts of commerce (‘eco-efficiency’), to a new paradigm of increasing its positive impacts (‘eco-effectiveness’). At its core, Cradle to Cradle design perceives the safe and productive processes of nature’s ‘biological metabolism’ as a model for developing a ‘technical metabolism’ flow of industrial materials. Product components can be designed for continuous recovery and reutilization as biological and technical nutrients within these metabolisms. For more information about MBDC and to obtain printable certificates for Eastman Copolyesters, visit http://www.mbdc.com.&& |
Product Description | |
---|---|
Supplier | Eastman |
Generic | PCTG |
Material Status | Commercial: Active |
Features | Good Clarity,High impact resistance,Low contractility,Good stripping performance,Solvent resistance |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.23 | g/cm³ | ASTM D792 |
optical performance | Nominal value | Unit | Test method |
---|---|---|---|
Transmittance | 92 | % | ASTM D1003 |
Haze μ M | 1.0 | % | ASTM D1003 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 73 | ℃ | ASTM D648 |
1.8 MPa, unannealed | 64 | ℃ | ASTM D648 |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
Dissipation factor | |||
Compared to the leakage tracing index | 600 | V | ASTM D3638 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame retardant level | |||
1.50mm | HB | UL-94 | |
3.00mm | HB | UL-94 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Impact strength of cantilever beam notch | |||
23℃ | NB | J/m | ASTM D256 |
-40℃ | 77 | J/m | ASTM D256 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Rockwell hardness | 105 | R 级 | ASTM D785 |
tensile strength | |||
23℃ | 44 | MPa | ASTM D638 |
Tensile strain | |||
Fracture, 23 ℃ | 330 | % | ASTM D638 |
Tensile modulus | |||
23℃ | 1800 | MPa | ASTM D638 |
bending strength | |||
23℃ | 66 | MPa | ASTM D790 |
Bending modulus | |||
23℃ | 1800 | MPa | ASTM D790 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 70 | °C | |
Drying time | 6.0 | Hr | |
Injection temperature | |||
Mold temperature | 20-40 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |