Tailored to meet the needs of injection-molding market, Eastar™ Copolyesters are clear materials with good mechanical properties and chemical resistance to a variety of substances. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®. The GREENGUARD INDOOR AIR QUALITY CERTIFIED® Mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products.&&

Product Description
SupplierEastman
Generic PCTG
Material StatusCommercial: Active
FeaturesSolvent resistance
AvailabilitysNorth America

Technical Data
PHYSICALNominal valueUnitTest method
Density1.33g/cm³ASTM D792
Shrinkage rate
MD0.20%ASTM D955
Water absorption rate
23℃,24hr0.19%ASTM D570

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch ASTM D256
-40℃33J/mASTM D256
23℃56J/mASTM D256
Impact strength of cantilever beam notch ASTM D4218
-40℃2400J/mASTM D4218
23℃No Break ASTM D4218
Dart impact equipped with measuring instruments ASTM D3763
-40℃,Energy @ Max. Load38.0JASTM D3763
23℃,Energy @ Max. Load32.0JASTM D3763

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed63.0ASTM D648
0.45 MPa, unannealed69.0ASTM D648
Vicat Softening Temp80.0ASTM D1525 2

optical performanceNominal valueUnitTest method
Transmittance
total82.0%ASTM D1003
Haze< 1.0%ASTM D1003

MECHANICALNominal valueUnitTest method
tensile strength
Fracture, 23 ℃24.0MPaASTM D638
Yield, 23 ℃58.0MPaASTM D638
Tensile strain
Fracture, 23 ℃90%ASTM D638
Yield, 23 ℃4.0%ASTM D638
Bending modulus
23℃2400MPaASTM D790
bending strength
23℃78.0MPaASTM D790
Rockwell hardness
R-level111 ASTM D785

Process Conditions
injectionNominal valueUnitTest method
Drying temperature160°C
Drying time4.0 to 6.0hr
Processing (melt) temperature277 to 293°C
Mold temperature16 to 32°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. Loading 1 (10 N)
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.