Meets ISO 10993 and/or USP Class VI biocompatibility requirement. Eastar™ Copolyester MN211, Natural contains a mold release for improved ejection. It is a brilliantly clear polymer with good impact strength, chemical resistance, dimensional stability, and low shrinkage rates. The slower rate of crystallization of this material makes it excellent for use in hot runner systems with valve or thermal gates. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED The GREENGUARD INDOOR AIR QUALITY CERTIFIED Mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products.&&

Product Description
SupplierEastman
Generic PCTG
Material StatusCommercial: Active
FeaturesGood Clarity,High impact resistance,Good Dimensional Stability,Low contractility,E-beam disinfection,Good stripping performance,Good color stability,Radiation disinfection,Solvent resistance
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.27g/cm³ASTM D792
Shrinkage rate
MD:3.2 mm0.20 to 0.50%ASTM D955
Water absorption rate
23℃,24hr0.13%ASTM D570

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch ASTM D256
-40℃37J/mASTM D256
23℃100J/mASTM D256
Impact strength of cantilever beam notch ASTM D4218
-40℃No Break ASTM D4218
23℃No Break ASTM D4218

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed63.0ASTM D648
0.45 MPa, unannealed70.0ASTM D648
Vicat Softening Temp85.0ASTM D1525
specific heat ASTM D2766
60℃1300J/kg/℃ASTM D2766
240℃2010J/kg/℃ASTM D2766
Thermal conductivity coefficient
23℃0.19W/m/K

optical performanceNominal valueUnitTest method
Transmittance ASTM D1003
total91.0%ASTM D1003
Regular88.0%ASTM D1003
Haze0.30%ASTM D1003

MECHANICALNominal valueUnitTest method
tensile strength
Fracture, 23 ℃28.0MPaASTM D638
Yield, 23 ℃50.0MPaASTM D638
Tensile strain
Fracture, 23 ℃110%ASTM D638
Yield, 23 ℃4.3%ASTM D638
Bending modulus
23℃2100MPaASTM D790
bending strength
23℃70.0MPaASTM D790
Rockwell hardness
R-level106 ASTM D785

Process Conditions
injectionNominal valueUnitTest method
Drying temperature71°C
Drying time4.0 to 6.0hr
Processing (melt) temperature249 to 271°C
Mold temperature16 to 38°C

Notes
1. Typical properties: these are not to be construed as specifications.
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.