Ecoflex® Supersoft 00-10

About
Ecoflex® rubbers are platinum-catalyzed silicones that are versatile and easy to use. Ecoflex® rubbers are mixed 1A:1B by weight or volume and cured at room temperature with negligible shrinkage. Low viscosity ensures easy mixing and de-airing, or you can choose to mix and dispense using our convenient dispensing cartridges. Cured material is skin safe and certified by an independent laboratory to ISO 10993-10, Biological evaluation of medical devices, Part 10: Tests for irritation and skin sensitization. Cured rubber is very soft, very strong and very “stretchy”, stretching many times its original size without tearing and will rebound to its original form without distortion. Ecoflex® rubbers are water white translucent and can be color pigmented with Silc Pig® pigments for creating a variety of color effects. You can also add Smooth-On’s Silicone Thinner® to further lower the viscosity. THI-VEX® silicone thickener can be added by weight to Ecoflex® silicones for brushable aplications. Soft, Softer, Softest . .Ecoflex® rubbers are based on Smooth-On’s Dragon Skin® technology and are currently available in four different hardness’: Shore A-5, Shore 00-10, 00-20, 00-30 and 00-50. They are suitable for a variety of applications including making prosthetic appliances, cushioning for orthotics and special effects applications (especially in animatronics where repetitive motion is required). Ecoflex® 5 has a pot life of 1 minute and a demold time of 5 minutes – Available only in dispensing cartridges. Note: Ecoflex® 00-10 cures with a “tacky” surface.&&

Product Description
Generic硅酮
Material StatusCommercial: Active
FeaturesGood Rigidity,Low Viscosity,Low contractility,Good Tensile Strength,Good tear strength,Soft
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe
Process Methodscasting

Technical Data
PHYSICALNominal valueUnitTest method
Density1.04g/cm³ASTM D1475
Specific volume0.961cm³/gASTM D1475
Shrinkage rate
MD< 0.10%ASTM D2566

MECHANICALNominal valueUnitTest method
Shore hardness
Shaw’s OO10 ASTM D2240

elastic bodyNominal valueUnitTest method
tensile strength
fracture0.827MPaASTM D412
100% strain0.0552MPaASTM D412
Tensile strain
fracture800%ASTM D412
tear strength3.85kN/mASTM D624

Electrical performanceNominal valueUnitTest method
Dielectric strength> 14kV/mmASTM D149

THERMALNominal valueUnitTest method
storage stability30minASTM D2471
Thermosetting mixed viscosity14000cPASTM D2393
stripping time240min

Supplementary informationNominal valueUnitTest method
Mixing ratio1A:1B by volume 
working temperature-54 to 232

Notes
1. Typical properties: these are not to be construed as specifications.
2. Die B
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.