About |
---|
Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms. Typical applications Cable jackets, plugs and terminations, spiral tubing, Films, ski-boot shells, ear tags, technical mouldings like mining screens, railway pads, seals.&& |
Product Description | |
---|---|
Supplier | BASF |
Material Status | Commercial: Active |
Features | Low temperature toughness,Antimicrobial properties,Hydrolysis stability |
Availabilitys | Europe |
Process Methods | Injection Molding,Extrusion |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.08 | g/cm³ | ISO 1183/A |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shore A, 3 seconds | 71 | ISO 7619 | |
Abrasion Loss | < 50.0 | mm³ | ISO 4649-A |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile Strength | |||
Yield yld | 30.0 | MPa | DIN 53504 |
4.80 | MPa | DIN 53504 | |
20% strain | 1.30 | MPa | DIN 53504 |
100% strain strain | 2.00 | MPa | DIN 53504 |
Tensile Strain | |||
Broken BRK | 850 | % | DIN 53504 |
Tear strength | 44 | kN/m | ISO 34-1 |
ISO 815 | |||
23℃,72 hr | 24 | % | ISO 815 |
70℃,24 hr | 50 | % | ISO 815 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-30℃ | No Break | ISO 179 | |
23℃ | No Break | ISO 179 |
Process Conditions | |||
---|---|---|---|
Extrusion Molded | Nominal value | Unit | Test method |
Injection Molding | Nominal value | Unit | Test method |
Melt Temperature | 160 to 220 | °C | |
Melt Temperature | 170 to 240 | °C | |
Mold Temperature | 20 to 70 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. Method Bb, Angle (Nicked) |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |