EMERGE™ 8230-20 advanced resin is an opaque, ignition resistant PC resin that contains no chlorinated or brominated or phosphorous based additives. This resin combines good mechanical and high heat properties and maintains excellent processability and contains mold release agent. EMERGE 8230-20 has a UL 94 V-0 rating at 1.5mm and is UV stabilized. Applications: Meters Electrical applications&& |
Product Description | |
---|---|
Supplier | Trinseo |
Generic | Polycarbonate |
Material Status | Commercial: Active |
Features | Excellent Processability,Halogen free,Flame Characteristics,High Heat Resistance,V-0 |
Availabilitys | Asia Pacific |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.20 | g/cm³ | ISO 1183/B |
Melt Flow Rate | |||
300℃,1.20kg | 20 | g/10min | ISO 1133 |
Shrinkage rate | |||
MD | 0.50 to 0.70 | % | ISO 294-4 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | |||
4 mm, injection molded | 2400 | MPa | ISO 527-2/50 |
tensile strength | |||
Yield, 4 mm, injection molding | 60.0 | MPa | ISO 527-2 |
Fracture, 4 mm, injection molded | 58.0 | MPa | ISO 527-2/50 |
Tensile strain | |||
Fracture, 4 mm, injection molded | 100 | % | ISO 527-2/50 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | |||
23 ℃, injection molding | 12 | kJ/m² | ISO 179/1eA |
Impact strength of cantilever beam notch | |||
3.2mm, injection molded | 750 | J/m | ISO 180 |
23 ℃, injection molding | 11 | kJ/m² | ISO 180-A |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.8 MPa, unannealed | 125 | ℃ | ISO 75-2/A |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame retardant level | |||
1.50 mm | V-0 | UL 94 | |
Glowing wire flammability index | IEC 60695-2-12 | ||
1.0 mm | 960 | ℃ | IEC 60695-2-12 |
2.0 mm | 960 | ℃ | IEC 60695-2-12 |
3.0 mm | 960 | ℃ | IEC 60695-2-12 |
optical performance | Nominal value | Unit | Test method |
---|---|---|---|
Transmittance | 87.0 to 91.0 | % | ASTM D1003 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 120 | °C | |
Drying time | 3.0 to 4.0 | hr | |
Processing (melt) temperature | 260 to 300 | °C | |
Mold temperature | 70 to 100 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. This rating not intended to reflect hazards presented by this or any other material under actual fire conditions. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |