About |
---|
75 Shore A TPE (Styrenic Block Copolymer based) for injection molding and extrusion applications. This grade offers soft/tactile feel and adhesion (overmolding) to Nylon.&& |
Product Description | |
---|---|
Generic | TPE |
Material Status | Commercial: Negative |
Features | Weather resistance is good,Excellent Processability,Alkali resistant,High elastic,Renewable resources,Ethanol tolerance,Acidproof,Good bond,Grease resistance,Ozone resistance,Solvent resistance,Soft,Good coloring,Resistance to detergents |
Availabilitys | North America |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.948 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
230℃,2.16kg | 6.5 | g/10min | ASTM D1238 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | ASTM D2240 | ||
Shore A, 10 seconds, extrusion molding | 71 | ASTM D2240 | |
Shore A, 10 seconds, injection molding | 75 | ASTM D2240 |
elastic body | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
fracture | 6.03 | MPa | ASTM D412 |
100% strain | 2.69 | MPa | ASTM D412 |
Tensile strain | |||
fracture | 400 | % | ASTM D412 |
tear strength | 35.0 | kN/m | ASTM D624 |
Compression deformation | ASTM D395B | ||
23℃,22 hr | 27 | % | ASTM D395B |
70℃,22 hr | 48 | % | ASTM D395B |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Embrittlement temperature | -52.0 | ℃ | ASTM D746 |
Dynamic Service Temperature | 90 | ℃ |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Extrusion | Nominal value | Unit | Test method |
Drying temperature | 60 to 70 | °C | |
Drying time | 2.0 to 3.0 | hr | |
Barrel rear temperature | 171 to 199 | °C | |
Barrel middle temperature | 229 to 241 | °C | |
Barrel front temperature | 241 to 249 | °C | |
Nozzle temperature | 221 to 241 | °C | |
Processing (melt) temperature | 229 to 249 | °C | |
Mold temperature | 10 to 49 | °C | |
Injection pressure | 5.17 to 8.96 | MPa | |
Drying temperature | 60 to 70 | °C | |
Drying time | 2.0 to 3.0 | hr | |
Barrel temperature | 160 to 179 | °C | |
Barrel 1 zone temperature | 229 to 241 | °C | |
Barrel 3 zone temperature | 241 to 249 | °C | |
Barrel 5 zone temperature | 241 to 249 | °C | |
Connector temperature | 229 to 249 | °C | |
Melt temperature | 229 to 249 | °C | |
Nozzle temperature | 229 to 249 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |