ENVIROLOY® ENV15-NC390

About
Injection Molding Grade, Non-Halogenated – Non-Chlorinated Flame Retardant, UV Stabilized, w/Mold Release, Good Heat Resistance, RoHS Compliant NC390 = To Be Assigned 5 Digit Number Indicating Natural, Black, or Custom Color. Contact Enviroplas Regarding UL Recognized Versions Of This Product.&&

Product Description
GenericPC+ABS
Material StatusCommercial: Active
FeaturesWeather resistance is good,Halogen free,Good stripping performance,Flame Characteristics,High Heat Resistance,V-0,5VA
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.18g/cm³ASTM D792
Melt Flow Rate ASTM D1238
240℃,5.0kg16g/10minASTM D1238
260℃,5.0kg22g/10minASTM D1238
Shrinkage rate
MD0.40 to 0.70%ASTM D955

MECHANICALNominal valueUnitTest method
tensile strength
yield60.7MPaASTM D638
Tensile strain
fracture40%ASTM D638
Bending modulus2380MPaASTM D790
bending strength89.6MPaASTM D790

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch
23℃530J/mASTM D256

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed90.6ASTM D648

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant level Internal Method
1.50 mmV-0 Internal Method
3.00 mm5VA Internal Method

Process Conditions
injectionNominal valueUnitTest method
Drying temperature82°C
Drying time3.0 to 4.0hr
Recommended maximum moisture content0.050%
Barrel rear temperature249 to 277°C
Barrel middle temperature249 to 277°C
Barrel front temperature254 to 288°C
Nozzle temperature249 to 271°C
Mold temperature66 to 93°C

Notes
1. Typical properties: these are not to be construed as specifications.
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.