FLEX NORYL™ Resin WCA105

About
Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requirements as defined by UL 1581. 56 Shore D hardness. Excellent processing using standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.&&

Product Description
SupplierSABIC
GenericPPO(PPE)+TPE
Material StatusCommercial: Active
FeaturesExcellent Processability,Good flexibility,Halogen free,Flame Characteristics
AvailabilitysNorth America

Technical Data
PHYSICALNominal valueUnitTest method
Density1.03g/cm³ASTM D792
Melt Flow Rate
250℃,10.0kg5.1g/10minASTM D1238
Water absorption rate
23℃,48hr0.10%ASTM D570

elastic bodyNominal valueUnitTest method
tear strength25kN/mISO 6383

THERMALNominal valueUnitTest method
Hot deformation temperature
0.45 MPa, unannealed, 6.4 mm85.0ASTM D648
Embrittlement temperature< -40.0ASTM D746
Vicat Softening Temp
A50102ISO 306/A50
UL temperature rating105UL 1581
Heat Deformation(121℃)26%UL 1581

Electrical performanceNominal valueUnitTest method
Volume resistivity3.9E+16ohms·cmIEC 60093
Dielectric strength
2 mm in oil26kV/mmIEC 60243-1
Relative permittivity
50 Hz2.60 
60 Hz2.60 
1 MHz2.50 
Dissipation factor
50 Hz0.024 
60 Hz0.024 
1 MHz3.8E-3 
Compared to the leakage tracing index600VIEC 60112

FLAME CHARACTERISTICSNominal valueUnitTest method
Glowing wire flammability index
3.0 mm960IEC 60695-2-12
Igniting temperature of the hot wire
3 mm750IEC 60695-2-13
Extreme oxygen index25%ISO 4589-2
VW-1Pass UL 1581
Smoke density
Flaming,Ds max:500.0 µm150 
Non-Flaming,Ds max:500.0 µm75 

MECHANICALNominal valueUnitTest method
Shore hardness
Shaw’s D56 ISO 868
tensile strength
fracture33.0MPaUL 1581
fracture23.0MPaASTM D638
Fracture, 136 ℃36.0MPaUL 1581
fracture23.0MPaISO 527-2/50
Tensile strain
fracture200%UL 1581
fracture85%ASTM D638
Fracture, 136 ℃160%UL 1581
fracture90%ISO 527-2/50
Bending modulus
100 mm span650MPaASTM D790
720MPaISO 178

Process Conditions
Squeeze descriptionNominal valueUnitTest method

Notes
1. Typical properties: these are not to be construed as specifications.
2. 2.0 mm wire with 0.12 mm x 20 stranded copper
3. Type I, 2.0 in/min
4. After 7 days. Tested on 2.0 mm wire with 0.12 mm x 20 stranded copper
5. 6 days, 2.0 mm wire with 0.12 mm x 20 stranded copper
6. 0.49 in/min
7. 2.0mm wire with 0.12 mm x 20 stranded copper
8. 250g, 2.0 mm wire with 0.12 mm x 20 stranded copper
9. Plaque
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.