Fortron® ICE 504L

About
FORTRON ICE 504L is a 40% glass fiber reinforced material that belongs to our new generation of PPS. This new technology allows you to optimize your molding conditions with faster cycle times for complex shapes or process with low mold temperatures.&&

Product Description
SupplierCelanese
GenericPPS
Material StatusCommercial: Active
FeaturesQuick molding cycle,V-0
AvailabilitysNorth America,Europe

Technical Data
IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength ISO 179/1eA
-30℃10kJ/m²ISO 179/1eA
23℃10kJ/m²ISO 179/1eA
Charpy Unnotch Impact strength ISO 179/1eU
-30℃53kJ/m²ISO 179/1eU
23℃53kJ/m²ISO 179/1eU
Impact strength of cantilever beam notch ISO 180/1A
-30℃10kJ/m²ISO 180-1A
23℃10kJ/m²ISO 180-1A
Notched impact strength of cantilever beam
23℃34kJ/m²ISO 180/1U

THERMALNominal valueUnitTest method
Hot deformation temperature
8.0 MPa, unannealed215ISO 75-2/C
1.8 MPa, unannealed270ISO 75-2/A
Glass transition temperature90.0ISO 11357-2
Melting temperature280ISO 11357-3
Linear coefficient of thermal expansion
TD4.2E-51/℃ISO 11359-2
MD2.6E-51/℃ISO 11359-2

Electrical performanceNominal valueUnitTest method
Surface resistivity> 1.0E+15ohmsIEC 60093
Volume resistivity> 1.0E+15ohms·cmIEC 60093
Dielectric strength28kV/mmIEC 60243-1
Relative permittivity
1 MHz4.60 IEC 60250
Dissipation factor
1 MHz6.2E-3 IEC 60250
Compared to the leakage tracing index125VIEC 60112

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant level UL 94
0.38 mmV-0 UL 94
1.50 mmV-0 UL 94
Extreme oxygen index47%ISO 4589-2

MECHANICALNominal valueUnitTest method
Tensile modulus14700MPaISO 527-2/1A/1
tensile strength
fracture195MPaISO 527-2/1A/5
Tensile strain
fracture1.9%ISO 527-2/1A/5
Bending modulus
23℃14500MPaISO 178
bending strength285MPaISO 178
Rockwell hardness
M-level100 ISO 2039-2

PHYSICALNominal valueUnitTest method
Density1.65g/cm³ISO 1183
Shrinkage rate ISO 294-4
TD0.40 to 0.60%ISO 294-4
MD0.20 to 0.60%ISO 294-4
Water absorption rate
Saturation, 23 ℃0.020%ISO 62
Melt Specific Heat1500J/kg/℃Internal Method

Process Conditions
injectionNominal valueUnitTest method
Drying temperature130 to 140°C
Drying time3.0 to 4.0hr
Recommended maximum moisture content0.020%
Hopper temperature20 to 30°C
Barrel rear temperature290 to 300°C
Barrel middle temperature310 to 320°C
Barrel front temperature330 to 340°C
Nozzle temperature310 to 330°C
Processing (melt) temperature330 to 340°C
Mold temperature90 to 160°C
Injection pressure50.0 to 100MPa
Injection speedFast 
Hold pressure30.0 to 70.0MPa
Back pressure0.00 to 3.00MPa

Notes
1. Typical properties: these are not to be construed as specifications.
2. 10°C/min
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.