Supplier | EMS-GRIVORY |
Generic | PA66/6 |
Material Status | Commercial: Active |
Features | V-0,low-temperature impact resistance,High impact resistance,Good Rigidity,Good flexibility,Impact copolymer |
Availabilitys | Europe,Asia Pacific,Africa & Middle East |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
MECHANICAL | Nominal value | Unit | Test method |
Tensile Modulus | |||
Dry | 3600 | MPa | ISO 527 |
Wet Cond | 1600 | MPa | ISO 527 |
Tensile Stress | |||
Yield yld, dry dry dry | 85 | MPa | ISO 527 |
Yield yld, wet cond | 50 | MPa | ISO 527 |
Broken BRK, dry dry | 75 | MPa | ISO 527 |
Broken BRK, wet Cond | 100 | MPa | ISO 527 |
Tensile Strain | |||
Yield yld, dry dry dry | 4 | % | ISO 527 |
Yield yld, wet cond | 15 | % | ISO 527 |
Broken BRK, dry dry | 10 | % | ISO 527 |
Broken BRK, wet Cond | >50 | % | ISO 527 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Unnotch Impact strength | |||
23 ℃, dry | 75 | kJ/m² | ISO 179/1eU |
23 ℃, moist cond | 100 | kJ/m² | ISO 179/1eU |
-30 ℃, dry | 70 | kJ/m² | ISO 179/1eU |
Charpy Notched Impact Strength | |||
23 ℃, dry | 4 | kJ/m² | ISO 179/1eA |
23 ℃, moist cond | 15 | kJ/m² | ISO 179/1eA |
-30 ℃, dry | 3 | kJ/m² | ISO 179/1eA |
-30 ℃, moist cond | 3 | kJ/m² | ISO 179/1eA |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Melting temperature | 260 | ℃ | ISO 11357-3 |
Hot deformation temperature HDT | |||
1.8 MPa | 70 | ℃ | ISO 75-1/-2 |
0.45 MPa | 210 | ℃ | ISO 75-1/-2 |
Coeff. of linear thermal expansion | |||
Parallel | 70 | E-6/K | ISO 11359-2 |
Normal | 90 | E-6/K | ISO 11359-2 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame Class Rating | |||
1.5 mm | V-0 | UL 94 | |
0.4 mm | V-0 | UL 94 | |
Oxygen Index | 35 | % | ISO 4589-2 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Maximum usage temperature | |||
Long term | 100-120 | °C | ISO 2578 |
Short term | 200 | °C | ESM |
ELECTRICAL | Nominal value | Unit | Test method |
---|---|---|---|
Relative permittivity | |||
100 Hz, dry | 3 | IEC 60250 | |
100 Hz, moist cond | 8 | IEC 60250 | |
1 MHz, dry | 3 | IEC 60250 | |
1 MHz, moist cond | 4 | IEC 60250 | |
Dissipation Factor | |||
100 Hz, dry | 50 | E-4 | IEC 60250 |
100 Hz, moist cond | 1500 | E-4 | IEC 60250 |
1 MHz, dry | 150 | E-4 | IEC 60250 |
1 MHz, moist cond | 700 | E-4 | IEC 60250 |
Volume Resistance | |||
Dry | 1E11 | ohm·m | IEC 60093 |
Wet Cond | 1E9 | ohm·m | IEC 60093 |
Surface Resistivity | 1E10 | ohm | IEC 60093 |
Electric strength | |||
Dry | 28 | kV/mm | IEC 60243-1 |
Wet Cond | 26 | kV/mm | IEC 60243-1 |
Compared Tracking Index | 600 | IEC 60112 |
PHYSICAL | Nominal value | Unit | Test method |
---|---|---|---|
Water Absorption | 8 | % | ISO 62 |
Moisture Absorption | 2.5 | % | ISO 62 |
Density | 1160 | kg/m³ | ISO 1183 |
Molding shrinkage | |||
Parallel | 0.7 | % | ISO 294-4 |
Normal | 0.8 | % | ISO 294-4 |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |