| About |
|---|
| Halar® 2408DA is a filled, pearl-white, semicrystalline melt processable fluorinated resin that may be used in full compliance with the federal Food, Drug, and Cosmetic Act. It is designed for electrostatic powder coatings and is particularly recommended for use in protection and anti-corrosion applications where food contact compliance is required. Halar® 2408DA provides superior water vapor permeation resistance compared to Halar® 6014. It also exhibits very good chemical, electrical and thermal properties. Additionally Halar® 2408DA coatings show very good surface finish and hardness. Main features of Halar® 2408DA include: Food contact compliance Very good chemical resistance Very good thermal properties Optimum permeation resistance Outstanding flame resistance Very good surface characteristics Purity&& |
| Product Description | |
|---|---|
| Supplier | Solvay |
| Generic | ECTFE |
| Material Status | Commercial: Active |
| Features | High purity,Good surface appearance,Good Electrical Properties,Good Hardness,Corrosion Resistant,Food contact compliance,Hypocrystalline,Solvent resistance,Heat Stabilized |
| Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.68 | g/cm³ | ASTM D3275 |
| Melt Flow Rate | |||
| 275℃,2.16kg | 12 | g/10min | ASTM D3275 |
| Average particle size | 80 | µm | Internal Method |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Melting temperature | 227 | ℃ | ASTM D3275 |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |