About |
---|
Ingeo 4060D, a product from NatureWorks LLC, can be coextruded with other Ingeo resin to form a sealant layer for biaxially oriented Ingeo film. This resin has excellent heat seal and hot tack performance with a seal initiation temperature of 80°C. This sealant does not adversely affect the unique properties of Ingeo bixially oriented film such as high gloss and transparency, dead-fold or aroma and grease barrier.&& |
Product Description | |
---|---|
Generic | PLA |
Material Status | Commercial: Active |
Features | Good surface appearance,Good heat sealing,High elastic,Renewable resources,Biodegradable,Food contact compliance,Grease resistance |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.24 | g/cm³ | ASTM D1505 |
film | Nominal value | Unit | Test method |
---|---|---|---|
Initial sealing temperature | 80.0 | ℃ | ASTM F88 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Glass transition temperature | 55.0 to 60.0 | ℃ | ASTM D3417 |
optical performance | Nominal value | Unit | Test method |
---|---|---|---|
gloss | |||
20° | 90 | ASTM D1003 | |
Haze | 2.0 | % | ASTM D1003 |
Process Conditions | |||
---|---|---|---|
Extrusion | Nominal value | Unit | Test method |
Drying temperature | 43 | °C | |
Drying time | 4.0 | hr | |
Recommended maximum moisture content | 0.025 | % | |
Barrel 1 zone temperature | 179 | °C | |
Barrel 2 zone temperature | 191 | °C | |
Barrel 3 zone temperature | 199 | °C | |
Connector temperature | 199 | °C | |
Melt temperature | 210 | °C | |
Nozzle temperature | 191 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |