About |
---|
Product Description | |
---|---|
Supplier | Mitsubishi |
Generic | Polycarbonate |
Material Status | Commercial: Negative |
Features | High liquidity,Good stability,weathering resistance |
Availabilitys | Asia Pacific,North America,Latin America,Europe,Africa & Middle East |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.2 | g/cm³ | ISO 1183 |
Melt Flow Rate | |||
300℃,1.2 kg | 30 | g/10min | ISO 1133 |
Melt Volume Rate | |||
300℃,1.2 kg | 28 | cm³/10min | ISO 1133 |
Shrinkage rate | |||
vertical | 0.5-0.7 | % | 内部 |
flow | 0.5-0.7 | % | 内部 |
Water Absorption | |||
24 h,23℃ | 0.24 | % | 内部 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile Modulus | 2400 | MPa | ISO 527 |
Tensile Stress | |||
Yield yld | 62 | MPa | ISO 527 |
Tensile Strain | |||
Yield yld | 6.6 | % | ISO 527 |
Broken BRK | 120 | % | ISO 527 |
Flexural Modulus | 2300 | MPa | ISO 178 |
Flexural Stress | 93 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | 50 | kJ/m² | ISO 179 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature HDT | |||
0.45 MPa | 136 | ℃ | ISO 75-1/-2 |
1.8 MPa | 123 | ℃ | ISO 75-1/-2 |
Coeff. of linear thermal expansion | |||
flow | 6.5E-5 | cm/cm/℃ | ISO 11359-2 |
vertical | 6.6E-5 | cm/cm/℃ | ISO 11359-2 |
ELECTRICAL | Nominal value | Unit | Test method |
---|---|---|---|
Surface Resistivity | 6E15 | ohms | IEC 60093 |
Volume Resistance | 3E16 | ohms·cm | IEC 60093 |
Dielectric Strength | |||
1.00 mm | 31 | kV/mm | IEC 60243-1 |
3.00 mm | 18 | kV/mm | IEC 60243-1 |
Dielectric Constant | |||
1 MHz | 3.1 | IEC 60250 | |
100 MHz | 3.1 | IEC 60250 | |
Dissipation Factor | |||
1 MHz | 9E-3 | IEC 60250 | |
100 MHz | 6E-4 | IEC 60250 | |
Compared Tracking Index | 2 | PLC Code | UL 746 |
Process Conditions | |||
---|---|---|---|
Injection Molding | Nominal value | Unit | Test method |
Drying Temperature | 120 | ℃ | |
Drying Time | 4.0-8.0 | hr | |
Rear Temperature Zone 1 | 270-290 | ℃ | |
Middle Temperature Zone 2 | 270-290 | ℃ | |
Front Temperature Zone 3 | 270-290 | ℃ | |
Nozzle temperature | 270-290 | ℃ | |
Mold Temperature | 70-100 | ℃ |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |