| About |
|---|
| Kynar Flex® resins are fluorinated thermoplastic copolymers. Kynar Flex® 2850 PC resin powder coating is a semi-crystalline copolymer of vinylidene fluoride and hexafluoropropylene. It has a special particle size making it ideal for spray applied powder coating on metal substrates for abrasion and corrosion protection&& |
| Product Description | |
|---|---|
| Supplier | Arkema |
| Generic | PVDF |
| Material Status | Commercial: Active |
| Features | Corrosion Resistant,Hypocrystalline,Good wear resistance |
| Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.78 | g/cm³ | ISO 1183 |
| Melt Volume Rate | |||
| 230℃,3.8 kg | 7.50 | cm³/10min | ISO 1133 |
| Water absorption rate | |||
| Saturation, 23 ℃ | 0.030 | % | ISO 62 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | |||
| yield | 35.0 | MPa | ISO 527-2 |
| Tensile strain | |||
| yield | 10 | % | ISO 527-2 |
| Nominal tensile fracture strain | > 50 | % | ISO 527-2 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Hot deformation temperature | |||
| 1.8 MPa, unannealed | 46.0 | ℃ | ISO 75-2/A |
| Melting temperature | 158 | ℃ | ISO 11357-3 |
| Electrical performance | Nominal value | Unit | Test method |
|---|---|---|---|
| Volume resistivity | 2.0E+14 | ohms·cm | IEC 60093 |
| FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
|---|---|---|---|
| Extreme oxygen index | 43 | % | ISO 4589-2 |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 2. 10°C/min |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |