About |
---|
LEXAN EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers improved ductility over conventional GF reinforced PC resins in combination with medium flow characteristics and excellent processability with opportunities for shorter IM cycle times when compared to standard PC. LEXAN EXL4019 resin is a product that may be an excellent candidate for a wide variety of applications. Available in limited colors only.&& |
Product Description | |
---|---|
Supplier | SABIC |
Generic | Polycarbonate |
Material Status | Commercial: Active |
Features | Good Rigidity,Excellent Processability,Ductility,Quick molding cycle,Moderate liquidity,Copolymer,HB |
Availabilitys | North America,Asia Pacific |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.25 | g/cm³ | ASTM D792 |
Density | 1.25 | g/cm³ | ISO 1183 |
Melt Flow Rate | |||
300℃,1.20kg | 7.5 | g/10min | ASTM D1238 |
Melt Volume Rate | |||
300℃,1.2 kg | 6.50 | cm³/10min | ISO 1133 |
Shrinkage rate | |||
TD:3.2 mm | 0.20 to 0.60 | % | Internal Method |
MD:3.2 mm | 0.20 to 0.60 | % | Internal Method |
Water absorption rate | |||
Saturation, 23 ℃ | 0.15 | % | ISO 62 |
Equilibrium, 23 ℃, 50% RH | 0.40 | % | ISO 62 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | 3950 | MPa | ASTM D638 |
Tensile modulus | 3900 | MPa | ISO 527-1-2 |
tensile strength | |||
fracture | 48.0 | MPa | ISO 527-2/5 |
fracture | 45.0 | MPa | ASTM D638 |
yield | 55.0 | MPa | ASTM D638 |
yield | 54.0 | MPa | ISO 527-2/5 |
Tensile strain | |||
fracture | 8.7 | % | ISO 527-2/5 |
fracture | 14 | % | ASTM D638 |
yield | 4.3 | % | ASTM D638 |
yield | 4.3 | % | ISO 527-2/5 |
Bending modulus | 3450 | MPa | ISO 178 |
50 mm span | 3500 | MPa | ASTM D790 |
bending strength | 98.0 | MPa | ISO 178 |
bending strength | |||
Yield, 50 mm span | 103 | MPa | ASTM D790 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | ||
-30℃ | 15 | kJ/m² | ISO 179/1eA |
23℃ | 25 | kJ/m² | ISO 179/1eA |
Charpy Unnotch Impact strength | ISO 179/1eU | ||
-30℃ | No Break | ISO 179/1eU | |
23℃ | No Break | ISO 179/1eU | |
Impact strength of cantilever beam notch | ASTM D256 | ||
-30℃ | 150 | J/m | ASTM D256 |
23℃ | 350 | J/m | ASTM D256 |
Impact strength of cantilever beam notch | ISO 180/1A | ||
-30℃ | 10 | kJ/m² | ISO 180-1A |
23℃ | 25 | kJ/m² | ISO 180-1A |
Notched impact strength of cantilever beam | ISO 180/1U | ||
-30℃ | No Break | ISO 180/1U | |
23℃ | No Break | ISO 180/1U | |
Dart impact equipped with measuring instruments | |||
23℃,Total Energy | 40.0 | J | ASTM D3763 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.8 MPa, unannealed, 3.2 mm | 137 | ℃ | ASTM D648 |
1.8 MPa, unannealed, 100 mm span | 135 | ℃ | ISO 75-2/Ae |
Vicat Softening Temp | 146 | ℃ | ASTM D1525 10 |
Vicat Softening Temp | |||
B50 | 146 | ℃ | ISO 306 |
B120 | 146 | ℃ | ISO 306/B120 |
Ball pressure test | |||
75℃ | Pass | IEC 60695-10-2 | |
Linear coefficient of thermal expansion | |||
TD:-40~40℃ | 7.0E-5 | 1/℃ | ASTM E831 |
TD:-40~40℃ | 7.0E-5 | 1/℃ | ISO 11359-2 |
MD:-40~40℃ | 4.7E-5 | 1/℃ | ISO 11359-2 |
MD:-40~40℃ | 4.7E-5 | 1/℃ | ASTM E831 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame retardant level | |||
0.75 mm | HB | UL 94 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 121 | °C | |
Drying time | 3.0 to 4.0 | hr | |
Drying time, maximum | 48 | hr | |
Recommended maximum moisture content | 0.020 | % | |
Recommended injection volume | 40 to 60 | % | |
Barrel rear temperature | 288 to 310 | °C | |
Barrel middle temperature | 299 to 321 | °C | |
Barrel front temperature | 310 to 332 | °C | |
Nozzle temperature | 304 to 327 | °C | |
Processing (melt) temperature | 310 to 332 | °C | |
Mold temperature | 82 to 116 | °C | |
Back pressure | 0.345 to 0.689 | MPa | |
Screw speed | 40 to 70 | rpm | |
Vent depth | 0.025 to 0.076 | mm |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. 0.20 in/min |
3. Type I, 0.20 in/min |
4. 0.051 in/min |
5. 0.079 in/min |
6. at Yield |
7. 80*10*3 sp=62mm |
8. 80*10*3 mm |
9. 120*10*4 mm |
10. Rate A (50°C/h), Loading 2 (50 N) |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |