LEXAN™ ML144R resin

About
中等粘度,多用途聚碳酸酯树脂,增加了脱模剂,食品接触级的只适用有限的颜色,从2007年1月15日起,这一等级将不再受生物相容性信息的支持,也不应被用于要求生物相容性的医学应用。供替代的选择有 HP3REU。

Product Description
SupplierSABIC
GenericPolycarbonate
Material StatusCommercial: Active
FeaturesGood stripping performance
AvailabilitysAfrica & Middle East ,Asia Pacific,Europe

Technical Data
MECHANICALNominal valueUnitTest method
Taber wear and tear
CS-17,1 kg10mg/1000cyInternal Method
tensile strength
Fracture, Type I, 50 mm/min70MPaISO 527
Yield, Type I, 50 mm/min63MPaISO 527
Tensile strain
Fracture, Type I, 50 mm/min110%ISO 527
Yield, Type I, 50 mm/min6%ISO 527
Tensile modulus
1 mm/min2350MPaISO 527
bending strength
Yield, 2 mm/min90MPaISO 178
Bending modulus
2 mm/mim2300MPaISO 178
Rockwell hardness (H358/30)95MPaISO 2039-1

IMPACTNominal valueUnitTest method
Notched impact strength of cantilever beam
23℃,80*10*3NBkJ/m²
Notched impact strength of cantilever beam
-30℃,80*10*3NBkJ/m²
Impact strength of cantilever beam notch
-30℃,80*10*370kJ/m²
-30℃,80*10*312kJ/m²
Impact strength of cantilever beam notch
Notched impact strength of cantilever beam
23℃,80*10*4NBkJ/m²
Notched impact strength of cantilever beam
-30℃,80*10*4NBkJ/m²
Charpy Notched Impact Strength
-30℃,80*10*3NBkJ/m²
-30℃,80*10*314kJ/m²
23℃,80*10*3NBkJ/m²
23℃,80*10*373kJ/m²
Charpy Notched Impact Strength
23℃35kJ/m²
Charpy Unnotch Impact strength
23 ℃, 80 * 10 * 4, 62 mm spanNBkJ/m²
-30 ℃, 80 * 10 * 4, 62 mm spanNBkJ/m²

THERMALNominal valueUnitTest method
Thermal conductivity coefficient0.2W/m/℃ISO 8302
Linear coefficient of thermal expansion
MD:-23~80℃7.E-051/℃ISO 11359-2
Ball pressure test 125 ℃+/-2 ℃PASSESIEC 60695-10-2
Ball pressure test
Maximum approximation value140IEC 60695-10-2
Vicat Softening Temp141ISO 306
A50153ISO 306
Vicat Softening Temp142ISO 306
Hot deformation temperature
1.8 MPa, 64 mm span125ISO 75/Be
0.45 MPa, 64 mm span136ISO 75/Be
Relative temperature index
Non mechanical impact performance125UL 746
Electrical performance130UL 746
Impact mechanical performance125UL 746

PHYSICALNominal valueUnitTest method
Shrinkage rate
MD0.5 – 0.7%Internal Method
Density1.2g/cm³ISO 1183
Water absorption rate
23℃,50% RH0.15%ISO 62
Saturation, 23 ℃0.35%ISO 62
Melt Volume Rate
300℃,1.2 kg12cm³/10minISO 1133

optical performanceNominal valueUnitTest method
Transmittance
2.54 mm88 – 90%ASTM D1003
Haze
2.54 mm<0.8%ASTM D1003
Refractive index1.586ISO 489

Electrical performanceNominal valueUnitTest method
Volume resistivity>1.E+15ohms·cmIEC 60093
Surface resistivity
ROA> 1.E +15ohmsIEC 60093
Insulation strength
Short term, 1.0mm15kV/mmIEC 60243-1
In oil, 3.2 mm17kV/mmIEC 60243-1
Relative permittivity
50-60 Hz2.7IEC 60250
1 MHz2.7IEC 60250
Dissipation factor
50-60 Hz0.001IEC 60250
1 MHz0.01IEC 60250

FLAME CHARACTERISTICSNominal valueUnitTest method
94HB flame rating assessment1.5mmUL 94
94HB flame level 2nd reference value3mmUL 94
Glowing wire flammability index
850 ℃, passed through1mmIEC 60695-2-12
Extreme oxygen index
LOI25%ISO 4589

Process Conditions
injection moldingNominal valueUnitTest method
Drying temperature 120 °C
Drying time 2 – 4 hrs
Maximum water content 0.02 %
Melt temperature 280 – 310 °C
Nozzle temperature 270 – 290 °C
Front Section Zone 3 Temperature 280 – 310 °C
Temperature in Zone 2 of the middle section 270 – 290 °C
Temperature in Zone 1 of the rear section 260 – 280 °C
Hopper temperature 60 – 80 °C
Mold temperature 80 – 110 °C

Notes
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.