LNP™ LUBRICOMP™ OCP36 compound

About
LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Internally Lubricated, Bearing Grade, Electrically Conductive.&&

Product Description
SupplierSABIC
GenericPPS
Material StatusCommercial: Active
FeaturesConductive,Lubricating
AvailabilitysNorth America,Asia Pacific
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.51g/cm³ASTM D792
Density1.54g/cm³ISO 1183
Shrinkage rate
TD:24 hrs0.40 to 0.60%ASTM D955
MD:24 hrs0.20 to 0.30%ASTM D955
Water absorption rate
Equilibrium, 23 ℃, 50% RH0.029%ISO 62
24hr,50% RH0.022%ASTM D570

MECHANICALNominal valueUnitTest method
Tensile modulus26100MPaASTM D638
Tensile modulus24900MPaISO 527-1-2
tensile strength
fracture166MPaISO 527-2/5
fracture165MPaASTM D638
Tensile strain
fracture0.90%ISO 527-2/5
fracture0.90%ASTM D638
Bending modulus22200MPaISO 178
50 mm span21400MPaASTM D790
bending strength254MPaISO 178
Fracture, 50 mm span253MPaASTM D790
friction coefficient ASTM D3702 Modified
dynamic0.47 ASTM D3702 Modified
static state0.33 ASTM D3702 Modified
Wear factor
Washer24.010^-10 in^5-min/ft-lb-hrASTM D3702 Modified

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch
23℃4.8kJ/m²ISO 180-1A
23℃490J/mASTM D4812
23℃53J/mASTM D256
Notched impact strength of cantilever beam
23℃26kJ/m²ISO 180/1U
Multi axial instrumented impact energy0.420JISO 6603-2

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed, 64 mm span266ISO 75-2/Af
1.8 MPa, unannealed, 3.2 mm260ASTM D648
0.45 MPa, unannealed, 64 mm span278ISO 75-2/Bf
0.45 MPa, unannealed, 3.2 mm279ASTM D648

Electrical performanceNominal valueUnitTest method
Surface resistivity1.0E+2ohmsASTM D257

Process Conditions
injectionNominal valueUnitTest method
Drying temperature121 to 149°C
Drying time4.0hr
Barrel rear temperature304 to 316°C
Barrel middle temperature321 to 332°C
Barrel front temperature332 to 343°C
Processing (melt) temperature316 to 321°C
Mold temperature138 to 166°C
Back pressure0.172 to 0.344MPa
Screw speed30 to 60rpm

Notes
1. Typical properties: these are not to be construed as specifications.
2. 0,20 in/min
3. Type I, 0,20 in/min
4. 0,051 in/min
5. 0,079 in/min
6. Modified: Manual
7. 80*10*4 mm
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.