About |
---|
Lupolen 4261 AG BD is a high molecular weight high density polyethylene (HDPE). Typical customer applications include automotive fuel tank applications if outstanding biodiesel durability is requested. It is supplied in pellets and is stabilized with antioxidants for the extrusion process. The product features an outstanding Environmental Stress Cracking Resistance (ESCR), good chemical resistance in combination with an excellent low temperature impact resistance. Typical processes include blow molding and thermoforming. Physical properties and process ability are very close to Lupolen 4261 AG. Lupolen 4261 AG BD is not intended for use in medical and pharmaceutical applications. The product can not be used for food contact applications.&& |
Product Description | |
---|---|
Supplier | LyondellBasell |
Generic | HMW-HDPE |
Material Status | Commercial: Active |
Features | High impact resistance,Inoxidizability,High molecular weight,Solvent resistance,low-temperature impact resistance,High ESCR,Fuel resistance |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Process Methods | Extrusion |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.945 | g/cm³ | ISO 1183 |
Apparent density | > 0.50 | g/cm³ | ISO 60 |
Melt Flow Rate | |||
190℃,21.6kg | 6.0 | g/10min | ISO 1133 |
ESCR(Environmental Stress Cracking Resistance) | 1000 | hr | ASTM D1693B |
Full incision creep test | |||
3.5 MPa,80℃ | 3.3 | day | ISO 16770 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | 900 | MPa | ISO 527-2 |
tensile strength | |||
yield | 24.0 | MPa | ISO 527-2 |
Tensile strain | |||
yield | 10 | % | ISO 527-2 |
Bending modulus | 1100 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Tensile impact strength | ISO 8256/1A | ||
-30℃ | 170 | kJ/m² | ISO 8256/1A |
23℃ | 250 | kJ/m² | ISO 8256/1A |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Vicat Softening Temp | |||
A50 | 126 | ℃ | ISO 306/A50 |
Melting temperature | |||
DSC | 131 | ℃ | ISO 3146 |
Oxygen sensing time | |||
200℃ | 50 | min | ISO 11357-6 |
Process Conditions | |||
---|---|---|---|
Extrusion | Nominal value | Unit | Test method |
Melt temperature | 180 to 240 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. 2% Arkopal N100 |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |