About |
---|
LUVOCOM® 80-7580 is an Acetal (POM) Copolymer material filled with aramid fiber. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America for injection molding. Important attributes of LUVOCOM® 80-7580 are: High Dimensional Stability Lubricated Wear Resistant Typical applications include: Engineering/Industrial Parts Automotive Business/Office Goods Fabrics/Fibers&& |
Product Description | |
---|---|
Supplier | Lehmann |
Generic | Copolymer Polyformaldehyde |
Material Status | Commercial: Active |
Features | Good Dimensional Stability,Low coefficient of friction,Lubricating,Good wear resistance |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.46 | g/cm³ | ISO 1183 |
Melt Volume Rate | |||
190℃,5 kg | 14.0 | cm³/10min | ISO 1133 |
Shrinkage rate | 1.5 to 2.1 | % | DIN 16901 |
Water absorption rate | |||
23℃,24hr | < 0.10 | % |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | 2700 | MPa | ISO 527-2 |
tensile strength | |||
fracture | 45.0 | MPa | ISO 527-2 |
Tensile strain | |||
yield | 5.1 | % | ISO 527-2 |
Bending modulus | 2000 | MPa | ISO 178 |
bending strength | 65.0 | MPa | ISO 178 |
Bending strain | 6.4 | % | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | |||
23℃ | 2.8 | kJ/m² | ISO 179/1eA |
Charpy Unnotch Impact strength | |||
23℃ | 32 | kJ/m² | ISO 179/1fU |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Continuous use temperature | 100 | ℃ | UL 746B |
Maximum operating temperature | |||
short-term | 120 | ℃ |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
insulation resistance | > 1.0E+12 | ohms | IEC 60167 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | |||
Desiccant desiccant, B | 120 | °C | |
Hot air dryer, A | 75 | °C | |
Drying time | |||
Desiccant desiccant, B | 2.0 to 4.0 | hr | |
Hot air dryer, A | 2.0 to 8.0 | hr | |
Barrel rear temperature | 175 to 190 | °C | |
Barrel middle temperature | 185 to 205 | °C | |
Barrel front temperature | 180 to 200 | °C | |
Nozzle temperature | 175 to 200 | °C | |
Processing (melt) temperature | 200 | °C | |
Mold temperature | 80 to 120 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |