Makrolon® AL2647

About

Product Description
SupplierCovestro
GenericPolycarbonate
Material StatusCommercial: Active

Technical Data
PHYSICALNominal valueUnitTest method
Melt index (mass)
300℃;1.2Kg13g/10minISO 1133
Melt Index (Volume)
300℃;1.2Kg12cm³/10minISO 1133
Transparency rate
4mm>87%DIN 5036-1
2mm89%DIN 5036-1
3mm88%DIN 5036-1
1mm89%DIN 5036-1
Forming shrinkage rate0.6-0.8%ISO 1133
Refractive index1.587ISO 489
Viscosity coefficient56cm³/gISO 1628-4

MECHANICALNominal valueUnitTest method
Maximum penetration force
-30℃/2mm6400NISO 6603-2
23℃/2mm5400NISO 6603-2
Yield strain
50mm/min6.0%ISO 527
IZOD Notch Impact Strength
23℃85kJ/m²ISO 180-4A
-30℃12kJ/m²ISO 180-4A
Penetration energy
23℃/2mm60JISO 6603-2
-30℃/2mm65JISO 6603-2
Yield stress
50mm/min65MPaISO 527
CHARPY impact strength
-30℃NkJ/m²ISO 179-1eU
23℃NkJ/m²ISO 179-1eU
Tensile creep modulus
1000h1900MPaISO 899-1
1h2200MPaISO 899-1
Nominal tensile strain at fracture
50mm/min>50%ISO 527
Tensile modulus
1mm/min2400MPaISO 527

Other performanceNominal valueUnitTest method
Hygroscopicity
23 ℃/50% relative humidity0.12%ISO 62
Water absorption
0.30%ISO 62

Processing performanceNominal valueUnitTest method
Injection speed200mm/sISO 294

Basic performanceNominal valueUnitTest method
Haze
3.0mm<0.5%ISO 14782
Density1200Kg/m³ISO 1183

THERMALNominal valueUnitTest method
Hot deformation temperature
0.45MPa137ISO 75-2
1.80MPa125ISO 75-2
Vicat Softening Temp
50N;50℃/h143ISO 306
Mold temperature80ISO 294
Melt Temperature290ISO 294
Oxygen index28%ISO 4589-2
Glass transition temperature
10℃/min148ISO 11357-2

Electrical performanceNominal valueUnitTest method
Dielectric strength
1.0mm32KV/mmIEC 60243-1
tracking resistance
Solution A275等级/RatingIEC 60112
loss factor
1MHZ900.0001IEC 60250
100HZ50.0001IEC 60250
Surface resistivity1016ΩIEC 60093
Relative dielectric constant
1MHZ3.0IEC 60250
100HZ3.1IEC 60250
Volume resistivity1014Ω.mIEC 60093

Process Conditions
InjectionNominal valueUnitTest method
Melt Temperature280 – 320
Standard melt temperature300
Temperature of the feeding section of the material pipe250 – 270
Temperature of the middle section of the material pipe270 – 290
Temperature of the front section of the material pipe285 – 305
Nozzle temperature270 – 305
Mold temperature70 – 110
Maintaining pressure (actual maximum injection pressure)50 – 75%
Melt back pressure100 – 200bar
Screw speed0.05 – 0.2m/s
Injection volume30 – 70%
Drying temperature under dry air120
Drying time in dry air4h
Maximum moisture content≤0. 02%
Depth of exhaust groove0. 025 – 0. 075mm

Notes
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.