Halogen-free, low smoke, UV and ozone resistant, max. operating temperature 125°C, radiation cross-linkable, flame retardant compoundfor photovoltaic/solar cables for Green Energy/Solar applications.&& |
Product Description | |
---|---|
Generic | 热塑性聚酯 |
Material Status | Commercial: Active |
Features | Weather resistance is good,Low smoke,Crosslinked radiation,Halogen free,Flame Characteristics,High Heat Resistance,Ozone resistance |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Process Methods | Extrusion |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.50 | g/cm³ | ISO 1183/A |
Melt Flow Rate | |||
170℃,21.6kg | 23 | g/10min | ISO 1133 |
PH value | > 4.5 | EN 50267-2-2 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
thermosetting | IEC 540 | ||
Elongation under load | 15 | % | IEC 60540 |
Residual elongation | 5.0 | % | IEC 60540 |
Hot press test | |||
penetration 4h at 140℃ | 24 | % | IEC 811-3-1 |
Temperature index | 250 | ℃ | ASTM D2863 |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
Volume resistivity | EN 50395 | ||
20 ℃ | > 1.0E+14 | ohms·cm | EN 50395 |
90 ℃ | > 1.0E+11 | ohms·cm | EN 50395 |
Conductivity | < 10.0 | µS/mm |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Extreme oxygen index | 34 | % | ASTM D2863 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s D | 49 | ISO 7619 | |
tensile strength | IEC 811-1-1 | ||
— | 10.0 | MPa | IEC 811-1-1 |
— | 12.3 | MPa | IEC 811-1-1 |
Tensile strain | IEC 811-1-1 | ||
fracture | 230 | % | IEC 811-1-1 |
fracture | 160 | % | IEC 811-1-1 |
Fracture, -40 ℃ | > 30 | % | IEC 811-1-1 |
Process Conditions | |||
---|---|---|---|
Extrusion | Nominal value | Unit | Test method |
Barrel 1 zone temperature | 130 to 150 | °C | |
Barrel 2 zone temperature | 140 to 160 | °C | |
Barrel 3 zone temperature | 150 to 170 | °C | |
Barrel 4 zone temperature | 160 to 180 | °C | |
Barrel 5 zone temperature | 160 to 180 | °C | |
Connector temperature | 165 to 185 | °C | |
Head temperature | 170 to 190 | °C | |
Nozzle temperature | 170 to 190 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. After crosslinking |
3. Before crosslinking |
4. at 200°C/15min/0.2 MPa |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |