NORYL GTX™ Resin GTX9400W

About
High flow PPO+PA. Power distribution box applications.&&

Product Description
SupplierSABIC
GenericPPO(PPE)+PS+PA
Material StatusCommercial: Active
FeaturesHigh liquidity
AvailabilitysNorth America
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.10g/cm³ASTM D792
Melt Flow Rate
280℃,5.0kg97g/10minASTM D1238
Shrinkage rate
MD:3.2 mm1.2 to 1.4%
TD:3.2 mm1.1 to 1.4%

MECHANICALNominal valueUnitTest method
Tensile modulus1950MPaASTM D638
tensile strength
yield64.0MPaASTM D638
yield69.0MPaISO 527-2/50
fracture62.0MPaASTM D638
Tensile strain
yield11%ASTM D638
fracture40%ASTM D638
fracture39%ISO 527-2/5
Bending modulus
100 mm span2350MPaASTM D790
2700MPaISO 178
bending strength
Yield, 100 mm span100MPaASTM D790

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch
-30℃110J/mASTM D256
23℃260J/mASTM D256
-40℃13kJ/m²ISO 180-1A
-20℃15kJ/m²ISO 180-1A
23℃21kJ/m²ISO 180-1A
Notched impact strength of cantilever beam
-30℃770J/m
23℃850J/m
Dart impact equipped with measuring instruments
-30℃,Total Energy15.0J
23℃,Total Energy43.0J

THERMALNominal valueUnitTest method
Hot deformation temperature
0.45 MPa, unannealed, 3.2 mm190ASTM D648
0.45 MPa, unannealed, 6.4 mm202ASTM D648
0.45 MPa, unannealed, 4.0 mm, 64 mm span187ISO 75-2/Bf
1.8 MPa, unannealed, 3.2 mm83.0ASTM D648
1.8 MPa, unannealed, 6.4 mm170ASTM D648
1.8 MPa, unannealed, 4.0 mm, 64 mm span78.0ISO 75-2/Af
Vicat Softening Temp
212ASTM D1525 7
B50203ISO 306
Linear coefficient of thermal expansion
MD:-40~40℃1.2E-41/℃
TD:-40~40℃1.4E-41/℃

Process Conditions
injectionNominal valueUnitTest method
Drying temperature95 to 105°C
Drying time3.0 to 4.0hr
Recommended maximum moisture content0.070%
Recommended injection volume30 to 50%
Barrel rear temperature255 to 295°C
Barrel middle temperature260 to 295°C
Barrel front temperature265 to 295°C
Nozzle temperature270 to 295°C
Processing (melt) temperature270 to 295°C
Mold temperature65 to 95°C
Back pressure0.300 to 1.40MPa
Screw speed20 to 100rpm
Vent depth0.013 to 0.038mm

Notes
1. Typical properties: these are not to be construed as specifications.
2. 2.0 in/min
3. Type I, 2.0 in/min
4. 0.10 in/min
5. 0.079 in/min
6. 80*10*4 mm
7. Rate A (50°C/h), Loading 2 (50 N)
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.