NORYL™ Resin NH8006

About
NORYL NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptional balance of strength and dimensional stability. This grade can be processed via extrusion or injection molding. NORYL NH8006 is available in custom colors and may be an excellent material candidate for use in electrical and electronics markets.&&

Product Description
SupplierSABIC
GenericPPO(PPE)+PS
Material StatusCommercial: Active
FeaturesGood Rigidity,Good Dimensional Stability,Halogen free,Flame Characteristics
AvailabilitysNorth America
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density
1.33g/cm³ASTM D792
1.34g/cm³ISO 1183
Melt Flow Rate
280℃,5.0kg2.1g/10minASTM D1238
Melt Volume Rate
280℃,10 kg6.00cm³/10minISO 1133
Shrinkage rate
MD:3.2 mm0.20 to 0.25%Internal Method
Water absorption rate
Saturation, 23 ℃0.23%
Equilibrium, 23 ℃, 50% RH0.070%

MECHANICALNominal valueUnitTest method
Tensile modulus
9500MPaASTM D638
9000MPaISO 527-1-2
tensile strength
yield125MPaASTM D638
yield125MPaISO 527-2/5
fracture125MPaASTM D638
fracture125MPaISO 527-2/5
Tensile strain
yield2.0%ASTM D638
yield1.8%ISO 527-2/5
fracture2.0%ASTM D638
fracture1.8%ISO 527-2/5
Bending modulus
50 mm span8600MPaASTM D790
8000MPaISO 178
bending strength
160MPaISO 178
Yield, 50 mm span185MPaASTM D790

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
23℃9.0kJ/m²ISO 179/1eA
Impact strength of cantilever beam notch
-30℃75J/mASTM D256
23℃85J/mASTM D256
-30℃8.0kJ/m²ISO 180-1A
23℃8.0kJ/m²ISO 180-1A
Notched impact strength of cantilever beam
23℃500J/mASTM D4812
23℃26kJ/m²ISO 180/1U
Dart impact equipped with measuring instruments
23℃,Total Energy14.0JASTM D3763

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed, 3.2 mm149ASTM D648
1.8 MPa, unannealed, 4.0 mm, 64 mm span149ISO 75-2/Af
Vicat Softening Temp
156ASTM D1525 10
B120160ISO 306/B120
Linear coefficient of thermal expansion
MD:-40~40℃3.7E-51/℃ASTM E831
TD:-40~40℃5.5E-51/℃ASTM E831
TD:-40℃5.5E-51/℃ISO 11359-2
Relative temperature index110UL 746
Electrical performance110UL 746
Impact mechanical performance105UL 746

Electrical performanceNominal valueUnitTest method
Surface resistivity
> 4.0E+17ohmsASTM D257
4.0E+17 to 5.0E+17ohmsIEC 60093
Dielectric strength
3.2 mm in oil16kV/mmIEC 60243-1
Dielectric constant
1 MHz3.11 ASTM D150
1 MHz3.10 IEC 60250
Dissipation factor
1 MHz4.0E-3 ASTM D150
High Arc Burning Index (HAI)PLC 4 UL 746
High voltage arc marking rate
HVTRPLC 4 UL 746
Hot wire ignition
HWIPLC 0 UL 746

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant level
1.50 mmV-1 
2.00 mmV-0 
3.00 mm 
Glowing wire flammability index
3.2 mm960IEC 60695-2-12

Process Conditions
injectionNominal valueUnitTest method
Drying temperature110 to 120°C
Drying time2.0 to 3.0hr
Hopper temperature80 to 100°C
Barrel rear temperature260 to 280°C
Barrel middle temperature280 to 300°C
Barrel front temperature300 to 320°C
Nozzle temperature280 to 300°C
Processing (melt) temperature300 to 320°C
Mold temperature100 to 130°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. 0.20 in/min
3. Type I, 0.20 in/min
4. 0.051 in/min
5. 0.079 in/min
6. at Yield
7. 80*10*4 sp=62mm
8. 80*10*4 mm
9. Rate A (50°C/h), Loading 2 (50 N)
10. Surface
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.