The Petrothene GA501 series of resins is pelletized linear low density polyethylene selected by customers for film extrusion applications that require excellent drawdown and toughness. These resins have excellent puncture resistance, elongation and heat seal strength. Typical applications include heavy duty shipping sacks, trash can liners, commercial and industrial packaging, as well as food and consumer packaging. GA501 is available without additives or fully formulated with slip and antiblock additives.&& |
Product Description | |
---|---|
Supplier | LyondellBasell |
Generic | Linear low density polyethylene |
Material Status | Commercial: Active |
Features | Good flexibility,Good heat sealing,Smoothness,Good dissection,High anti-blocking,Food contact compliance,Puncture Resistant |
Availabilitys | North America,Latin America,Asia Pacific,Europe |
Process Methods | Film extrusion |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.918 | g/cm³ | ASTM D1505 |
Melt Flow Rate | |||
190℃,2.16kg | 1.0 | g/10min | ASTM D1238 |
film | Nominal value | Unit | Test method |
---|---|---|---|
film thickness | |||
test | 25 | µm | |
Secant modulus | |||
1% secant, TD, 25 µ m, blow molded film | 193 | MPa | ASTM D882 |
1% secant, MD, 25 µ m, blow molded film | 186 | MPa | ASTM D882 |
tensile strength | |||
TD, fracture, 25 µ m, blow molded film | 32.4 | MPa | ASTM D882 |
MD, fracture, 25 µ m, blow molded film | 45.5 | MPa | ASTM D882 |
Tensile strain | |||
TD, fracture, 25 µ m, blow molded film | 730 | % | ASTM D882 |
MD, fracture, 25 µ m, blow molded film | 580 | % | ASTM D882 |
Drop hammer impact | |||
25 µ m, blow molded film | 100 | g | ASTM D1709-A |
tear strength | |||
TD, 25 µ m, blow molded film | 330 | g | ASTM D1922 |
MD, 25 µ m, blow molded film | 130 | g | ASTM D1922 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Vicat Softening Temp | 107 | ℃ | ASTM D1525 |
optical performance | Nominal value | Unit | Test method |
---|---|---|---|
gloss | |||
45 °, 25.4 µ m, blow molded film | 40 | ASTM D2457 | |
Haze | |||
25.4 µ m, blow molded film | 20 | % | ASTM D1003 |
Supplementary information | Nominal value | Unit | Test method |
---|---|---|---|
Blow(up Ratio) | 2.5:1 |
Process Conditions | |||
---|---|---|---|
Extrusion | Nominal value | Unit | Test method |
Melt temperature | 204 to 232 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. 23°C |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |