| About |
|---|
| The PETROTHENE GA 601 series resins is pelletized, linear low density polyethylenes for applications that require maximum strength and toughness. These products offer excellent additive homogeneity, require no transfer equipment modifications, and facilitate clean and safe handling. Applications include heavy duty shipping sacks, prime liners, commercial and industrial packaging, as well as food and consumer packaging. The GA 601 series resins offers enhanced film strength, drawdown, toughness and heat seal strength. In addition, these resins have excellent low temperature resistance for applications such as stretch film and frozen food packaging. The GA 601 series resins can be purchased without additives, fully formulated with slip and antiblock or containing a processing aid.&& |
| Product Description | |
|---|---|
| Supplier | LyondellBasell |
| Generic | Linear low density polyethylene |
| Material Status | Commercial: Active |
| Features | Good Rigidity,Good flexibility,Good heat sealing,Good dissection,Food contact compliance |
| Availabilitys | North America,Latin America,Asia Pacific,Europe |
| Process Methods | Film extrusion |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 0.918 | g/cm³ | ASTM D1505 |
| Melt Flow Rate | |||
| 190℃,2.16kg | 1.0 | g/10min | ASTM D1238 |
| film | Nominal value | Unit | Test method |
|---|---|---|---|
| film thickness | |||
| test | 25 | µm | |
| Secant modulus | |||
| 1% secant, TD, 25 µ m | 224 | MPa | ASTM D882 |
| 1% secant, MD, 25 µ m | 200 | MPa | ASTM D882 |
| tensile strength | |||
| TD, fracture, 25 µ m | 42.1 | MPa | ASTM D882 |
| MD, fracture, 25 µ m | 55.8 | MPa | ASTM D882 |
| Tensile strain | |||
| TD, fracture, 25 µ m | 700 | % | ASTM D882 |
| MD, fracture, 25 µ m | 580 | % | ASTM D882 |
| Drop hammer impact | |||
| 25 µ m, blow molded film | 190 | g | ASTM D1709-A |
| Total energy impact | |||
| 25 µ m, blow molded film | 2.44 | J | ASTM D4272 |
| Elmandorf tear strength | |||
| MD,25 µm | 330 | g | ASTM D1922 |
| tear strength | |||
| TD,25 µm | 650 | g | ASTM D1922 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Vicat Softening Temp | 105 | ℃ | ASTM D1525 |
| optical performance | Nominal value | Unit | Test method |
|---|---|---|---|
| gloss | |||
| 45 °, 25.4 µ m, blow molded film | 35 | ASTM D2457 | |
| Haze | |||
| 25.4 µ m, blow molded film | 22 | % | ASTM D1003 |
| Process Conditions | |||
|---|---|---|---|
| Extrusion | Nominal value | Unit | Test method |
| Melt temperature | 204 to 232 | °C | |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |