About |
---|
PLEXIGLAS® XT rods and tubes are the clearest extruded tubes on the market today delivering brilliant quality, superior performance, and durability. PLEXIGLAS® XT rods and tubes are characterized by their flawless optics, and perfectly smooth surface free of striations. PLEXIGLAS® GS tubes are produced in the cast rotation process. Cast rods and square rods are made of casted semi-finished products. All cast forms have polished surfaces. Applications Due to the above characteristics PLEXIGLAS® rods and tubes are ideally suitable for. Architectural interior & exterior lighting. Contemporary furniture. Luxury brand merchandizing, store fixtures, P.O.P. & trade show displays Industrial pneumatic delivery and conveying systems Decorative architectural features&& |
Product Description | |
---|---|
Supplier | ROHM |
Generic | PMMA |
Material Status | Commercial: Active |
Features | Weather resistance is good,Good surface appearance,Renewable resources,Good Hardness,Machinable,Food contact compliance,Durability,Agglomerability |
Availabilitys | Europe |
Process Methods | Thermo forming |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.19 | g/cm³ | ISO 1183 |
Water absorption rate | |||
23℃,24hr | 41.0 | mg | ISO 62 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | 3300 | MPa | ISO 527-2 |
tensile strength | ISO 527-2/1B/5 | ||
-40℃ | 110 | MPa | ISO 527-2/1B/5 |
23℃ | 80.0 | MPa | ISO 527-2/1B/5 |
70℃ | 40.0 | MPa | ISO 527-2/1B/5 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Unnotch Impact strength | 15 | kJ/m² | ISO 179/1fU |
Impact strength of cantilever beam notch | 1.6 | kJ/m² | ISO 180-1A |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Vicat Softening Temp | 115 | ℃ | ISO 306/B |
Linear coefficient of thermal expansion | |||
MD:0~50℃ | 7.0E-5 | 1/℃ | DIN 53752-A |
Low temperature bending | |||
Minimum radius | 330 x thickness | ||
Maximum operating temperature | < 80 | ℃ |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Smoke Gas Corrosiveness | None | ||
Smoke Gas Volume | Very Low | DIN 4102 | |
Smoke Toxicity | None | DIN 53436 |
optical performance | Nominal value | Unit | Test method |
---|---|---|---|
Transmittance | 92.0 | % | DIN 5036 |
UV transmittance | No |
Supplementary information | Nominal value | Unit | Test method |
---|---|---|---|
Ignition Point | 425 | ℃ | DIN 51794 |
Surface Temperature(IRradiator) | < 200 | ℃ | |
Weight gain | |||
during immersion | < 2.1 | % | ISO 62 |
Forming temperature | |||
— | 160 to 175 | ℃ | |
Reverse | > 80 | ℃ |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |