Pro-fax SG702 high impact polypropylene copolymer is available in pellet form. This resin is typically used in injection molding applications and offers very good cold temperature impact resistance. An ASTM and ISO-based versions of the technical datasheet are available for Pro-fax SG702. For regulatory compliance information see Pro-fax SG702 Product Stewardship Bulletin (PSB).&& |
Product Description | |
---|---|
Supplier | LyondellBasell |
Generic | PP copolymer |
Material Status | Commercial: Active |
Features | low-temperature impact resistance,Impact copolymer |
Availabilitys | North America |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.898 | g/cm³ | ASTM D792-B |
Density | 0.900 | g/cm³ | ISO 1183 |
Melt Flow Rate | |||
230℃,2.16kg | 18 | g/10min | ASTM D1238 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
Yield, 23 ℃ | 19.0 | MPa | ISO 527-2 |
yield | 20.0 | MPa | ASTM D638 |
Tensile strain | |||
Yield, 23 ℃ | 6.0 | % | ISO 527-2 |
yield | 6.0 | % | ASTM D638 |
Bending modulus | |||
23℃ | 920 | MPa | ISO 178 |
1% secant | 1030 | MPa | ASTM D790-A |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-40℃ | 2.9 | kJ/m² | ISO 179 |
23℃ | 16 | kJ/m² | ISO 179 |
Impact strength of cantilever beam notch | ISO 180 | ||
23℃ | No Break | ASTM D256A | |
-40℃ | 5.0 | kJ/m² | ISO 180 |
23℃ | 42 | kJ/m² | ISO 180 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.8 MPa, unannealed | 49.0 | ℃ | ISO 75-2/A |
0.45 MPa, unannealed | 69.0 | ℃ | ISO 75-2/B |
0.45 MPa, unannealed | 82.2 | ℃ | ASTM D648 |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |