About |
---|
Standard injection moulding&& |
Product Description | |
---|---|
Supplier | Rondo |
Generic | PP not specified |
Material Status | Commercial: Active |
Features | HB |
Availabilitys | Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.940 | g/cm³ | ISO 1183 |
Melt Flow Rate | |||
230℃,2.16kg | 12 | g/10min | ISO 1133 |
Shrinkage rate | ISO 2577 | ||
TD | 1.2 to 1.6 | % | ISO 2577 |
MD | 1.2 to 1.6 | % | ISO 2577 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile strain | |||
yield | 8.0 | % | ISO 527-2 |
Bending modulus | |||
23℃ | 1100 | MPa | ISO 178 |
bending strength | 40.0 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20℃ | 3.0 | kJ/m² | ISO 179 |
23℃ | 8.0 | kJ/m² | ISO 179 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
1.60 mm | HB | UL 94 | |
Igniting temperature of the hot wire | |||
2 mm | 650 | ℃ | IEC 60695-2-13 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 80 | °C | |
Drying time | 2.0 to 4.0 | hr | |
Processing (melt) temperature | 180 to 220 | °C | |
Mold temperature | 40 to 80 | °C | |
Injection pressure | 40.0 to 110 | MPa |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |