Epalex 7575 HS UV1 is a thermoplastic rubber modified mineral filled polypropylene compound. It is a high flow injection moulding grade developed for high impact strength at sub-zero temperatures whilst maintaining good rigidity at high ambient temperatures. This material has been formulated to meet automotive heat ageing and interior UV requirements.&& |
Product Description | |
---|---|
Generic | PP not specified |
Material Status | Commercial: Active |
Features | Good Rigidity,Weather resistance is good,High impact resistance,High liquidity,low-temperature impact resistance,Heat Stabilized |
Availabilitys | Asia Pacific |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.10 | g/cm³ | ASTM D792 |
Shrinkage rate | |||
MD | 0.80-1.00 | % | ASTM D995 |
Melt Flow Rate | |||
230℃,2.16kg | 16 | g/10min | ASTM D1238 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 118 | ℃ | ASTM D648 |
Linear coefficient of thermal expansion | |||
MD | 0.000060 | 1/℃ | ASTM D696 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Impact strength of cantilever beam notch | |||
23℃ | 250 | J/m | ASTM D256 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s A | 73 | ASTM D2240 | |
Shore A15 seconds | 62 | ASTM D2240 | |
tensile strength | |||
23℃ | 11 | MPa | ASTM D638 |
Tensile strain | |||
Fracture, 23 ℃ | 200 | % | ASTM D638 |
Bending modulus | |||
23℃ | 2300 | MPa | ASTM D790 |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. 2.0 in/min |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |