| About |
|---|
| Cycoloy * CY4000树脂是一种可注塑,阻燃PC / ABS混合物,不含溴化或氯化阻燃添加剂。 Cycoloy CY4000具有出色的流动性和平衡冲击性能,可用于各种颜色选择。 它是各种不同应用的理想选择。 |
| Product Description | |
|---|---|
| Supplier | SABIC |
| Generic | PC+ABS |
| Material Status | Commercial: Active |
| Features | Halogen free |
| Availabilitys | Africa & Middle East ,North America,Asia Pacific,Europe |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.2 | g/cc | ISO 1183 |
| Shrinkage rate | |||
| MD | 0.4-0.6 | % | Internal Method |
| Melt Flow Rate | |||
| 260℃,2.16kg | 23 | g/10min | ASTM D1238 |
| 260℃,2.16kg | 21 | g/10min | ISO 1133 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Ball hardness | |||
| H358/30 | 110 | MPa | ISO 2039-1 |
| tensile strength | |||
| fracture | 45 | MPa | ISO 527 |
| yield | 55 | MPa | ISO 527 |
| Tensile strain | |||
| fracture | >= 40 | % | ISO 527 |
| yield | 3.0 | % | ISO 527 |
| Tensile modulus | 2700 | MPa | ISO 527 |
| bending strength | |||
| yield | 85 | MPa | ISO 178 |
| Bending modulus | 2500 | MPa | ISO 178 |
| Taber wear and tear | |||
| CS-17,1 kg | 15 | Internal Method |
| Electrical performance | Nominal value | Unit | Test method |
|---|---|---|---|
| Volume resistivity | >= 1.00e+15 | ohms·cm | IEC 60093 |
| Surface resistivity | ≧1.0E+15 | ohms | IEC 60093 |
| Dielectric constant | |||
| 1 MHz | 2.7 | IEC 60250 | |
| 50-60 Hz | 2.7 | IEC 60250 | |
| Dielectric strength | |||
| 3.2 mm in oil | 17.0 | kV/mm | IEC 60243-1 |
| Consumption factors | |||
| Frequency 50.0-60.0 Hz | 0.0060 | IEC 60250 | |
| Frequency 1.00e+6 Hz | 0.0060 | IEC 60250 | |
| Compared to the leakage tracing index | 600 | V | IEC 60112 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Linear coefficient of thermal expansion | |||
| parallel | 80.0 | µm/m-℃ | ISO 11359-2 |
| TD | 80.0 | µm/m-℃ | ISO 11359-2 |
| Hot deformation temperature | |||
| 0.45 MPa, 100 mm span | 85 | ℃ | ISO 75/Be |
| 1.8 MPa, 100 mm span | 72 | ℃ | ISO 75/Ae |
| Vicat Softening Temp | |||
| B50 | 85 | ℃ | ISO 306 |
| B120 | 90 | ℃ | ISO 306 |
| UL relative temperature index | |||
| Electrical performance | 60.0 | ℃ | UL 746B |
| Impact mechanical performance | 60.0 | ℃ | UL 746B |
| MECHANICAL | 60.0 | ℃ | UL 746B |
| Flame retardant level | |||
| 2.50 mm | V-0 | UL 94 | |
| Extreme oxygen index | 29 | % | ISO 4589 |
| Glowing wire flammability index | |||
| 3.2 mm | 960 | ℃ | IEC 60695-2-12 |
| IMPACT | Nominal value | Unit | Test method |
|---|---|---|---|
| Charpy Notched Impact Strength | |||
| -30℃ | 1 | kJ/m² | ISO 179/1eA |
| Impact strength of cantilever beam notch | |||
| -30℃ | 10 | kJ/m² | ISO 180/1A |
| Notes |
|---|
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |