| About |
|---|
| Salflex 364AH is a Thermoplastic Vulcanizate (TPV) product. It can be processed by injection molding and is available in North America. Applications of Salflex 364AH include automotive, engineering/industrial parts and bags/liners. Characteristics include: Fatigue Resistant Good Flexibility Good Tear Strength Impact Resistant&& |
| Product Description | |
|---|---|
| Generic | TPV |
| Material Status | Commercial: Active |
| Features | Good flexibility,High impact resistance,Fatigue resistance,Good tear strength,Ozone resistance |
| Availabilitys | North America |
| Process Methods | Injection Molding |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 0.920 | g/cm³ | ISO 1183/A |
| Shrinkage rate | 1.5 | % | ISO 294-4 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Shore hardness | |||
| Shore A, 15 seconds | 68 | ISO 868 |
| elastic body | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | |||
| fracture | 6.30 | MPa | ISO 37 |
| 100% strain | 3.50 | MPa | ISO 37 |
| Tensile strain | |||
| fracture | 500 | % | ISO 37 |
| tear strength | 31 | kN/m | ISO 34-1 |
| Compression deformation | |||
| 70℃,22 hr | 40 | % | ISO 815 |
| Aging performance | Nominal value | Unit | Test method |
|---|---|---|---|
| The rate of change in tensile strength in air | |||
| 125℃,1000 hr | -22 | % | ISO 188 |
| Changes in tensile stress during fracture in air | |||
| 125℃,1000 hr | -46 | % | ISO 188 |
| The rate of change of Shore hardness in air | |||
| Shaw A, 125 ℃, 1000 hr | -3.0 | ISO 188 | |
| The rate of change in tensile strength | |||
| 125 ℃, 168 hr, in IRM 903 oil | -38 | % | ISO 1817 |
| Changes in tensile stress during fracture | |||
| 125 ℃, 168 hr, in IRM 903 oil | -78 | % | ISO 1817 |
| Volume change | |||
| 125 ℃, 168 hr, in IRM 903 oil | 60 | % | ISO 1817 |
| Process Conditions | |||
|---|---|---|---|
| injection | Nominal value | Unit | Test method |
| Drying temperature | 60 to 75 | °C | |
| Drying time | 2.0 to 4.0 | hr | |
| Barrel rear temperature | 185 to 215 | °C | |
| Barrel middle temperature | 190 to 220 | °C | |
| Barrel front temperature | 190 to 220 | °C | |
| Nozzle temperature | 195 to 225 | °C | |
| Processing (melt) temperature | 195 to 215 | °C | |
| Mold temperature | 27 to 40 | °C | |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 2. Method Bb, Angle (Nicked) |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |