Santoprene™ 8201-70

About
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion, blow molding, thermoforming or vacuum forming. It is polyolefin based and recyclable within the manufacturing stream.&&

Product Description
SupplierCelanese
Material StatusCommercial: Active
FeaturesSoft,Halogen free,Block Copolymer,Good coloring,HB,Agglomerability,Weather resistance is good,Flame Characteristics
AvailabilitysEurope,North America,Asia Pacific,Africa & Middle East
Process MethodsExtrusion,Injection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density
0.948g/cm³ASTM D792
0.950g/cm³ISO 1183

MECHANICALNominal valueUnitTest method
Shore hardness
Shore A, 15 seconds, 23 ℃, 2.00 mm75ISO 868

elastic bodyNominal valueUnitTest method
tensile strength
TD, fracture, 23 ℃7.50MPaASTM D412, ISO 37
TD, 100% strain, 23 ℃2.90MPaASTM D412, ISO 37
Tensile strain
TD, fracture, 23 ℃570%ASTM D412,ISO 37
tear strength
TD,23℃26.0kN/mASTM D624
TD,23℃26kN/mISO 34-1
Compression deformation
70℃,22 hr36%ASTM D395B
125℃,70 hr57%ASTM D395B
70℃,22 hr36%ISO 815
125℃,70 hr57%ISO 815

Aging performanceNominal valueUnitTest method
The rate of change in tensile strength in air
150℃,168 hr-9.0%ASTM D573, ISO 188
The rate of change in ultimate elongation in air
150℃,168 hr-8.0%ASTM D573, ISO 188
The rate of change in hardness of a hardness tester in the air
Support A, 150 ℃, 168 hr2.0ASTM D573, ISO 188
Changes in air quality
150℃,168 hr-9.0%ISO 188
150℃,168 hr-9.0%ASTM D573
The rate of change in tensile strengthASTM D471, ISO 1817
23 ℃, 168 hr, in 15% sodium chloride-1.0%
23 ℃, 168 hr, in 50% sodium hydroxide-1.0%
23 ℃, 168 hr, in 98% sulfuric acid3.0%
23 ℃, 168 hr, in IRM 903 oil-14%
23 ℃, 168 hr, in water-6.0%
Change rate of ultimate elongationASTM D471, ISO 1817
23 ℃, 168 hr, in 15% sodium chloride-2.0%
23 ℃, 168 hr, in 50% sodium hydroxide2.0%
23 ℃, 168 hr, in 98% sulfuric acid4.0%
23 ℃, 168 hr, in IRM 903 oil-14%
23 ℃, 168 hr, in water8.0%
The rate of change in Shore hardness
Support A, 23 ℃, 168 hr, in 15% sodium chloride1.0ASTM D471
Support A, 23 ℃, 168 hr, in 50% sodium hydroxide1.0ASTM D471
Support A, 23 ℃, 168 hr, in 98% sulfuric acid-1.0ASTM D471
Support A, 23 ℃, 168 hr, in IRM 903 oil-14ASTM D471
Support A, 23 ℃, 168 hr, in water-1.0ASTM D471, ISO 1817
Support A, 23 ℃, 168 hr, in 15% sodium chloride1.0ISO 1817
Support A, 23 ℃, 168 hr, in 50% sodium hydroxide1.0ISO 1817
Support A, 23 ℃, 168 hr, in 98% sulfuric acid-1.0ISO 1817
Support A, 23 ℃, 168 hr, in IRM 903 oil-14ISO 1817
Quality change rateASTM D471
23 ℃, 168 hr, in 15% sodium chloride0.0%
23 ℃, 168 hr, in 50% sodium hydroxide0.0%
23 ℃, 168 hr, in 98% sulfuric acid1.0%
23 ℃, 168 hr, in IRM 903 oil48%
23 ℃, 168 hr, in water0.0%
Quality change rateISO 1817
23.0 ℃, 168 hr, in 50% sodium hydroxide0.0%
23.0 ℃, 168 hours in water0.0%
23.0 ℃, 168 hr, in 15% sodium chloride0.0%
23.0 ℃, 168 hr, in 98% sulfuric acid1.0%
23.0 ℃, 168 hr, in IRM 903 oil48%

THERMALNominal valueUnitTest method
Embrittlement temperature-63.0ASTM D746,ISO 812
Relative temperature indexUL 746
Electrical performance100UL 746
1.10 mm90.0
1.60 mm90.0
3.00 mm95.0

Electrical performanceNominal valueUnitTest method
Compared to the leakage tracing indexPLC 0UL 746
High Arc Burning Index (HAI)PLC 0UL 746
High voltage arc ignition resistance index (HVAR) (PLC)PLC 5UL 746
Hot wire ignition
HWIUL 746
1.60 mmPLC 3
3.00 mmPLC 2

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant levelUL 94
1.10 mmHB
1.60 mmHB
3.00 mmHB

Process Conditions
injectionNominal valueUnitTest method
ExtrusionNominal valueUnitTest method
Recommended maximum moisture content0.080%
Proposed maximum recycled material ratio20%
Barrel rear temperature179 to 196°C
Barrel middle temperature185 to 199°C
Barrel front temperature191 to 204°C
Nozzle temperature191 to 210°C
Processing (melt) temperature199 to 216°C
Mold temperature23.9 to 51.7°C
Injection speed快速
Back pressure0.345 to 0.689MPa
Screw speed100 to 200rpm
Clamping force4.1 to 6.9kN/cm²
Cushion3.18 to 6.35mm
Screw length to diameter ratio16.0:1.0 至 20.0:1.0
Screw compression ratio2.0:1.0 至 2.5:1.0
Vent depth0.025mm
Melt temperature185 to 221°C
Nozzle temperature185 to 221°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. Die C
3. Method Bb, Angle (Nicked)
4. Type 1
5. Type A
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.