| About |
|---|
| Sarlink TPV 24378N XRD is a high performance thermoplastic vulcanizate used in electrical and industrial applications. Sarlink TPV 24378N XRD is a high hardness, high density, flame retardant grade exhibiting superior sunlight resistance. This grade can be processed by injection molding and extrusion.&& |
| Product Description | |
|---|---|
| Supplier | Teknor Apex |
| Generic | TPV |
| Material Status | Commercial: Active |
| Features | Weather resistance is good,Low liquidity,Smoothness,Good Hardness,Flame Characteristics,High density,Halogenated,Bromination,Insulation,Good coloring |
| Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
| Process Methods | Injection Molding |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.29 | g/cm³ | ASTM D792 |
| Melt Flow Rate | |||
| 230℃,2.16kg | 0.50 | g/10min | ASTM D1238 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Shore hardness | |||
| Shaw’s A | 82 | ||
| Shore A, 5 seconds | 78 |
| elastic body | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | |||
| fracture | 6.21 | MPa | ASTM D412 |
| Tensile strain | |||
| fracture | 500 | % | ASTM D412 |
| FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
|---|---|---|---|
| Flame retardant level | |||
| 1.00 mm, natural color | V-2 | ||
| 1.50 mm, natural color | V-0 | ||
| Extreme oxygen index | 26 | % | ASTM D2863 |
| Legal Statement | Nominal value | Unit | Test method |
|---|---|---|---|
| Process Conditions | |||
|---|---|---|---|
| injection | Nominal value | Unit | Test method |
| Squeeze description | Nominal value | Unit | Test method |
| Extrusion | Nominal value | Unit | Test method |
| Barrel rear temperature | 199 to 210 | °C | |
| Barrel middle temperature | 204 to 216 | °C | |
| Barrel front temperature | 210 to 221 | °C | |
| Nozzle temperature | 216 to 227 | °C | |
| Processing (melt) temperature | 216 to 227 | °C | |
| Mold temperature | 35 to 66 | °C | |
| Injection pressure | 1.38 to 6.89 | MPa | |
| Injection speed | 快速 | ||
| Back pressure | 0.172 to 0.862 | MPa | |
| Screw speed | 50 to 120 | rpm | |
| Cushion | 3.81 to 25.4 | mm | |
| Barrel 1 zone temperature | 193 to 204 | °C | |
| Barrel 2 zone temperature | 199 to 210 | °C | |
| Barrel 3 zone temperature | 204 to 216 | °C | |
| Barrel 4 zone temperature | 207 to 218 | °C | |
| Barrel 5 zone temperature | 210 to 221 | °C | |
| Nozzle temperature | 216 to 227 | °C | |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |