SI-LINK™ DFDB-5445 BK is a RoHS (Reduction of Hazardous Substances)-compliant flame retardant masterbatch designed to be used in conjunction with SI-LINK™ DFDA-5451 NT Polyethylene and the catalyst masterbatch SI-LINK™ DFDB-5480 NT Polyethylene to form a flame retardant SI-LINK polyethylene insulation system. This system is bulletinized by UL as DFDB-5445 BK and is moisture curable. The specific gravity of the system is 1.02. It is recommended for use in low voltage power cable and industrial cable applications. It is formulated to pass the UL-44 horizontal burn test on larger cables. SI-LINK™ DFDB-5445 BK, a highly filled black flame retardant master-batch, is intended to be used at a 35% concentration along with 60% SI-LINK Polyethylene DFDA-5451 NT and 5% SI-LINK DFDB-5480 NT Catalyst Master-batch on size #2 AWG conductors and larger. At this concentration the requirements for XHH, XHHW, XHHW-2, RHH, RHW, RHW-2, SIS, USE and USE-2 cables as defined by UL-44, UL-854 are satisfied. . SI-LINK™ DFDB-5445 BK offers flexibility in tailoring the formulation to meet the horizontal burn requirement on a range of cable sizes. At increased concentrations, SI-LINK™ DFDB-5445 BK has been shown to provide horizontal burn test compliance in smaller sizes. The economics of the formulation may be optimized for a particular application depending on the cable sizes produced and the UL submittal sizes selected. Such factors as processing conditions, degree of cure and type of conductor can affect the results, so cable manufacturers must determine the optimal formulations for their applications. Recommendations are available upon request. SPECIFICATIONS The SI-LINK™ DFDB-5445 BK system is bulletinized by UL for XHH, XHHW, XHHW-2, RHH, RHW, RHW-2, SIS, USE and USE-2 on sizes 2 AWG and larger. It is suitable for CSA RW-90, and RWU-90 applications.&&

Product Description
SupplierDOW
GenericPE
Material StatusCommercial: Active
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe

Technical Data
PHYSICALNominal valueUnitTest method
Density1.02g/cm³ASTM D792

elastic bodyNominal valueUnitTest method
tensile strength13.8MPaASTM D412
Tensile strain
fracture300%ASTM D412

Aging performanceNominal valueUnitTest method
Change in Relative Permittivity UL 44
1-14 days1.0%UL 44
7-14 days-3.0%UL 44
Tensile strength retention rate
7 days,121℃80%ASTM D412
Elongation retention rate
7 days,121℃80%ASTM D412

THERMALNominal valueUnitTest method
thermal deformation
131℃< 15%UL 44
thermosetting
Elongation rate: 200 ℃< 50%IEC 60811-2-1

Electrical performanceNominal valueUnitTest method
Relative permittivity4.00 UL 44
Capacitance UL 44
pf,1 day:90℃950 UL 44
pf,14 days:90℃950 UL 44
pf,7 days:90℃950 UL 44

FLAME CHARACTERISTICSNominal valueUnitTest method
Extreme oxygen index26%ASTM D2863
Flame test
Horizontal,No. 4 AWG 60 mil wallPass UL 44

Supplementary informationNominal valueUnitTest method
Crushing Test5605NUL 44
Flexibility – 4 hrs(-25℃)No visible cracks UL 854

Notes
1. Typical properties: these are not to be construed as specifications.
2. 23°C
3. 15 min, 20N/cm²
4. 1 day. These tests were conducted on #14 AWG solid wires insulated with 0.030 in. wall thickness insulation.
5. These tests were conducted on #14 AWG solid wires insulated with 0.030 in. wall thickness insulation.
6. These tests were conducted on # 4 AWG stranded wire insulated with 0.060 in. wall thickness insulation.
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.