Stanyl® TW241F10

About
50% Glass Reinforced, Heat Stabilized, Lubricated&&

Product Description
SupplierDSM
GenericPA 46
Material StatusCommercial: Active
FeaturesHeat Stabilized
AvailabilitysEurope,Asia Pacific,North America

Technical Data
PHYSICALNominal valueUnitTest method
Density1620kg/m³ISO 1183
Water absorption rate1.85%ISO 62
Forming shrinkage rate
MD0.4%ISO 294-4
TD0.9%ISO 294-4

MECHANICALNominal valueUnitTest method
Tensile modulus
16000MPaISO 527-1/-2
120°C8500MPaISO 527-1/-2
160°C7200MPaISO 527-1/-2
180°C6600MPaISO 527-1/-2
200°C6000MPaISO 527-1/-2
Tensile stress
250MPaISO 527-1/-2
Fracture, 120 ° C140MPaISO 527-1/-2
Fracture, 160 ° C120MPaISO 527-1/-2
Fracture, 180 ° C110MPaISO 527-1/-2
Fracture, 200 ° C100MPaISO 527-1/-2
elongation at break2.7%ISO 527-1/-2
Tensile strain
Fracture, 120 ° C5%ISO 527-1/-2
Fracture, 160 ° C5.5%ISO 527-1/-2
Fracture, 180 ° C5.5%ISO 527-1/-2
Fracture, 200 ° C6%ISO 527-1/-2
Bending modulus
15000MPaISO 178
120°C7300MPaISO 178
160°C6500MPaISO 178
bending strength
380MPaISO 178
120°C180MPaISO 178
160°C150MPaISO 178

IMPACTNominal valueUnitTest method
Charpy Unnotch Impact strength
23°C100kJ/m²ISO 179/1eU
-30°C90kJ/m²ISO 179/1eU
Charpy Notched Impact Strength
23°C16kJ/m²ISO 179/1eA
-30°C14kJ/m²ISO 179/1eA
Impact strength of cantilever beam notch
23°C16kJ/m²ISO 180/1A
-40°C14kJ/m²ISO 180/1A

THERMALNominal valueUnitTest method
Melting temperature
10°C/min295ISO 11357-1/-3
Hot deformation temperature
1.80 MPa290ISO 75-1/-2
0.45 MPa290ISO 75-1/-2
Linear coefficient of thermal expansion
MD2.5E-5ISO 11359-1/-2
TD4.0E-5ISO 11359-1/-2
Relative temperature index
Electrical characteristics, 0.75mm65UL 746B
Heat index
5000 hrs177IEC 60216
5000 hrs177ISO 527-1/-2

Electrical performanceNominal valueUnitTest method
Volume resistivity1.0E+12ohms·cmIEC 62631-3-1
Dielectric strength30kV/mmIEC 62631-3-1
Compared to the leakage tracing index300VIEC 60112
Dielectric constant
100Hz4.3IEC 62631-2-1
1MHz4IEC 62631-2-1

Process Conditions
InjectionNominal valueUnitTest method
drying temperature80.0°C
Drying time4.0 to 8.0hr
Temperature at the rear of the barrel280 to 320°C
Temperature in the middle of the barrel300 to 320°C
Front temperature of material barrel300 to 320°C
Nozzle temperature300 to 320°C
Processing (melt) temperature305 to 320°C
Mold temperature80.0 to 120°C
Injection speed中等偏快
Back pressure2.00 to 10.0MPa
Screw compression ratio2.5:1.0

Notes
1. Typical properties: these are not to be construed as specifications.
2. 10°C/min
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.