SUMIKASUPER® LCP E4006L

About
SUMIKASUPER® LCP E4006L is a Liquid Crystal Polymer (LCP) material filled with glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Important attributes of SUMIKASUPER® LCP E4006L are: Flame Rated Heat Resistant Low Shrinkage&&

Product Description
SupplierSumitomo
Generic液态聚合物
Material StatusCommercial: Active
FeaturesGood Rigidity,Excellent Processability,Good heat aging resistance,Good Dimensional Stability,Low Viscosity,High Heat Resistance,Good bond,Solvent resistance,Welding,V-0
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.60g/cm³ASTM D792
Shrinkage rate Internal Method
MD0.11%Internal Method
TD0.78%Internal Method
Water absorption rate
saturated0.020%ASTM D570

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch
6.4mm140J/mASTM D256
Notched impact strength of cantilever beam
6.4 mm460J/mASTM D256

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed310ASTM D648
Linear coefficient of thermal expansion Internal Method
MD:150℃2.0E-61/℃Internal Method
TD:150℃8.1E-51/℃Internal Method
Thermal conductivity coefficient0.53W/m/KJIS R2618

Electrical performanceNominal valueUnitTest method
Volume resistivity1.0E+15ohms·cmASTM D257
Dielectric constant ASTM D150
1 kHz4.40 ASTM D150
1 MHz3.70 ASTM D150
Dissipation factor ASTM D150
1 kHz0.018 ASTM D150
1 MHz0.035 ASTM D150
Arc resistance130secASTM D495
Compared to the leakage tracing index185VIEC 60112

FLAME CHARACTERISTICSNominal valueUnitTest method
0.30 mmV-0 UL 94
Extreme oxygen index44%JIS K7201

Supplementary informationNominal valueUnitTest method
Soldering Resistance335Internal Method

MECHANICALNominal valueUnitTest method
Rockwell hardness
R-level91 ASTM D785
tensile strength
yield182MPaASTM D638
Tensile strain
fracture5.6%ASTM D638
Bending modulus ASTM D790
23℃11900MPaASTM D790
200℃5780MPaASTM D790
bending strength ASTM D790
Yield, 23 ℃155MPaASTM D790
Yield, 200 ℃47.0MPaASTM D790
shear strength58.0MPaASTM D732
Poisson’s ratio0.48 ASTM E132

Process Conditions
injectionNominal valueUnitTest method
Drying temperature120 to 150°C
Drying time3.0hr
Proposed maximum recycled material ratio30%
Barrel rear temperature330 to 350°C
Barrel middle temperature350 to 370°C
Barrel front temperature370 to 390°C
Nozzle temperature370 to 390°C
Processing (melt) temperature380°C
Mold temperature70 to 160°C
Injection pressure118 to 157MPa

Notes
1. Typical properties: these are not to be construed as specifications.
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.