| About |
|---|
| TPE 5345 is a flexible natural, olefin-based thermoplastic vulcanizate (TPV) intended for wire and cable insulation and jacketing applications where high temperature performance and excellent flame resistance are required. TPE 5345 complies with “Restriction of Hazardous Substances” Directive, Citation 2002-95-EC, commonly known as RoHS without exemption. TPE 5345 exhibits excellent wet and dry electrical properties and superior chemical resistance. It also provides good resistance to abrasion, impact and crush. TPE 5345 also exhibits superior low temperature properties as demonstrated by it passing cold bend and impact testing at -40°C. TPE 5345 contains a halogen-based, flame retardant additive package designed to reduce normal PE flame spread characteristics. It also offers good extrusion processing characteristics on either conventional polyethylene or PVC extrusion lines. TPE 5345 is readily pigmented to a variety of colors using standard wire and cable color concentrates designed for thermoplastic or crosslinked polyolefins. UV light standards can be met with the addition of carbon black UV masterbatch.&& |
| Product Description | |
|---|---|
| Generic | TPV |
| Material Status | Commercial: Active |
| Features | Good flexibility,High impact resistance,Good Electrical Properties,Flame Characteristics,Good wear resistance,Solvent resistance,Halogenated |
| Availabilitys | North America |
| Process Methods | Extrusion |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.17 | g/cm³ | ASTM D792 |
| elastic body | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | |||
| 0.762 mm | 16.5 | MPa | ASTM D412 |
| Tensile strain | |||
| Fracture, 0.762 mm | 600 | % | ASTM D412 |
| Aging performance | Nominal value | Unit | Test method |
|---|---|---|---|
| Tensile strength retention rate | |||
| 7 days at 136℃,762.0 µm | 90 | % | UL 1581 |
| Elongation retention rate | |||
| 7 days at 136℃,762.0 µm | 75 | % | UL 1581 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Embrittlement temperature | -40.0 | ℃ | ASTM D746 |
| Electrical performance | Nominal value | Unit | Test method |
|---|---|---|---|
| Volume resistivity | |||
| 1.91 mm | 1.6E+16 | ohms·cm | ASTM D257 |
| Dielectric strength | |||
| 1.91 mm | 26 | kV/mm | ASTM D149 |
| Dielectric constant | |||
| 1.91 mm,60 Hz | 2.40 | ASTM D150 | |
| Dissipation factor | |||
| 1.91 mm,60 Hz | 2.7E-3 | ASTM D150 |
| FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
|---|---|---|---|
| Extreme oxygen index | 25 | % | ASTM D2863 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Shore hardness | |||
| Shaw A, 0.762 mm | 92 | ASTM D2240 | |
| Bending modulus | |||
| 0.76 mm | 290 | MPa | ASTM D790 |
| Process Conditions | |||
|---|---|---|---|
| Extrusion | Nominal value | Unit | Test method |
| Drying temperature | 82 | °C | |
| Drying time | 3.0 | hr | |
| Barrel 1 zone temperature | 185 | °C | |
| Barrel 2 zone temperature | 193 | °C | |
| Barrel 3 zone temperature | 202 | °C | |
| Barrel 4 zone temperature | 213 | °C | |
| Melt temperature | 213 to 218 | °C | |
| Nozzle temperature | 216 | °C | |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |