About |
---|
TECAMID® 6/6 GF30 is a 30% glass-fiber reinforced nylon 6/6 material whose important properties include high tensile and flexural strength, stiffness, excellent heat deflection temperature, and superior abrasion and wear resistance. While all TECAMID® materials have high mechanical strength and superior resistance to wear and organic chemicals, TECAMID® 6/6 GF30 has more than double the strength and stiffness of unreinforced nylons and a heat deflection temperature which approaches its melting point. TECAMID® 6/6 GF30 has an excellent balance of properties which make it an ideal material for metal replacement in applications such as automotive parts, industrial valves, railway tie insulators, and other industry uses whose design requirements include high strength, toughness, and weight reduction. Superior organic chemical resistance High heat deflection temperature Excellent wear resistance Very good fatigue endurance Superior creep resistance&& |
Product Description | |
---|---|
Supplier | Ensinger |
Generic | PA66 |
Material Status | Commercial: Active |
Features | Good Rigidity,Good flexibility,Good Tensile Strength,Good wear resistance,Solvent resistance |
Availabilitys | North America |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.36 | g/cm³ | ASTM D792 |
Water absorption rate | |||
23℃,24hr | 0.25 | % | |
Saturation, 23 ℃ | 0.30 | % |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Notched impact strength of cantilever beam | |||
23℃ | 69 | J/m | ASTM D256 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Melting temperature | 259 | ℃ | |
Linear coefficient of thermal expansion | |||
MD | 4.9E-5 | 1/℃ | ASTM D696 |
specific heat | 1260 | J/kg/℃ | ASTM C351 |
Thermal conductivity coefficient | 0.39 | W/m/K | ASTM C177 |
Operating temperature | |||
Intermittent | 170 | ℃ | |
long-term | 110 | ℃ |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
Surface resistivity | 1.0E+14 | ohms | ASTM D257 |
Volume resistivity | 1.0E+14 | ohms·cm | ASTM D257 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Rockwell hardness | |||
M-level | 88 | ASTM D785 | |
Tensile modulus | |||
23℃ | 5520 | MPa | ASTM D638 |
tensile strength | |||
Yield, 23 ℃ | 93.1 | MPa | |
Fracture, 23 ℃ | 93.1 | MPa | |
Tensile strain | |||
Yield, 23 ℃ | 10 | % | |
Fracture, 23 ℃ | 10 | % | |
Bending modulus | |||
23℃ | 4830 | MPa | ASTM D790 |
bending strength | |||
23℃ | 135 | MPa | ASTM D790 |
Compression modulus | 2620 | MPa | ASTM D695 |
compressive strength | |||
10% strain, 23 ℃ | 117 | MPa | ASTM D695 |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |