TIPPLEN® K 693

About
TIPPLEN K 693 is a high molecular weight impact copolymer polypropylene for the extrusion and injection moulding applications. TIPPLEN K 693 offers excellent impact strength, good stiffness and excellent processability. TIPPLEN K 693 is recommended for medium-low weight corrugated cardboards, blow moulded bottles. This grade is also recommended for heavy-duty packaging and large containers. TIPPLEN K 693 is suitable for food contact. The product complies with Food Contact Regulations.&&

Product Description
GenericPP homopolymerization
Material StatusCommercial: Active
FeaturesGood Rigidity,Excellent Processability,High impact resistance,Renewable resources,Food contact compliance,High molecular weight,Impact copolymer
AvailabilitysEurope
Process MethodsExtrusion

Technical Data
PHYSICALNominal valueUnitTest method
Melt Flow Rate
230℃,2.16kg2.0g/10minISO 1133

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch ISO 180/A
-20 ℃, injection molding6.0kJ/m²ISO 180-A
23 ℃, injection molding25kJ/m²ISO 180-A

THERMALNominal valueUnitTest method
Hot deformation temperature
0.45 MPa, unannealed88.0ISO 75-2/B

MECHANICALNominal valueUnitTest method
Tensile modulus
injection molding1350MPaISO 527-2
tensile strength
Yield, injection molding29.0MPaISO 527-2
Tensile strain
Yield, injection molding8.0%ISO 527-2
Bending modulus
injection molding1450MPaISO 178
Rockwell hardness
R-level79 ISO 2039-2

Process Conditions
injectionNominal valueUnitTest method
ExtrusionNominal valueUnitTest method
Processing (melt) temperature190 to 240°C
Melt temperature190 to 240°C

Notes
1. Typical properties: these are not to be construed as specifications.
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.